Milić, Goran

Link to this page

Authority KeyName Variants
orcid::0000-0002-1144-0867
  • Milić, Goran (25)
Projects

Author's Bibliography

Walnut wood steaming: chemical profile and antioxidant activity of the condensate to assess the potential application

Milić, Goran; Rančić, Milica; Todorović, Nebojša; Zivanović, Nemanja; Orcić, Dejan; Simin, Natasa

(2024)

TY  - JOUR
AU  - Milić, Goran
AU  - Rančić, Milica
AU  - Todorović, Nebojša
AU  - Zivanović, Nemanja
AU  - Orcić, Dejan
AU  - Simin, Natasa
PY  - 2024
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/1461
AB  - Steaming of green timber, a common industrial process for various hardwood species, significantly influences wood properties, including coloration and drying characteristics. However, the environmental implications of substantial volumes of condensate generated during wood steaming underscore the urgency for its sustainable management. This study explores the chemical composition of the condensate obtained during the 90-hour indirect steaming of walnut timber (WTSC), aiming to identify potential applications for this wastewater while addressing environmental risks. Chemical characterization of WTSC included qualitative LC-MS/MS analysis, determination of the total phenolic content (TPC), total flavonoid content (TFC) and the content of selected phenolics. WTSC exhibited high TPC (188 mg gallic acid equivalents per L) and TFC (9.74 mg quercetin equivalents per L) values. Additionally, WTSC showed significant antioxidant activity (IC50 (DPPH) = 61.4 mu g/mL and 103 mu g ascorbic acid equivalents per mL in FRAP assay). Specific phenolic compounds detected in the WTSC distinguish it from other wood industry effluents and are a consequence of the unique characteristics of walnut wood and conditions during steaming process. A variety of acids (p-hydroxybenzoic, protocatechuic, syringic, gallic, cinnamic, cinnamic, p-coumaric, o-coumaric, vanillic) and flavonoids (apigenin, genistein, naringenin, luteolin, kaempferol, chrysoeriol, isorhamnetin, apigenin 7-O-glucoside, vitexin, kaempferol 3-O-glucoside, catechin, epicatechin, and quercitrin) were identified and quantified. The condensate exhibited higher TPC value and antioxidant activity than other wood industry effluents, positioning it as a promising natural antioxidant with potential applications in pharmaceutical and food industries. However, our short-term goal is to explore the potential use of WTSC as received - without isolating individual compounds - in studies focused on plant protection, textile dyeing, and wood-based panel production.
T2  - Wood Science and Technology
T1  - Walnut wood steaming: chemical profile and antioxidant activity of the condensate to assess the potential application
EP  - 1628
IS  - 4
SP  - 1605
VL  - 58
DO  - 10.1007/s00226-024-01584-9
UR  - conv_1807
ER  - 
@article{
author = "Milić, Goran and Rančić, Milica and Todorović, Nebojša and Zivanović, Nemanja and Orcić, Dejan and Simin, Natasa",
year = "2024",
abstract = "Steaming of green timber, a common industrial process for various hardwood species, significantly influences wood properties, including coloration and drying characteristics. However, the environmental implications of substantial volumes of condensate generated during wood steaming underscore the urgency for its sustainable management. This study explores the chemical composition of the condensate obtained during the 90-hour indirect steaming of walnut timber (WTSC), aiming to identify potential applications for this wastewater while addressing environmental risks. Chemical characterization of WTSC included qualitative LC-MS/MS analysis, determination of the total phenolic content (TPC), total flavonoid content (TFC) and the content of selected phenolics. WTSC exhibited high TPC (188 mg gallic acid equivalents per L) and TFC (9.74 mg quercetin equivalents per L) values. Additionally, WTSC showed significant antioxidant activity (IC50 (DPPH) = 61.4 mu g/mL and 103 mu g ascorbic acid equivalents per mL in FRAP assay). Specific phenolic compounds detected in the WTSC distinguish it from other wood industry effluents and are a consequence of the unique characteristics of walnut wood and conditions during steaming process. A variety of acids (p-hydroxybenzoic, protocatechuic, syringic, gallic, cinnamic, cinnamic, p-coumaric, o-coumaric, vanillic) and flavonoids (apigenin, genistein, naringenin, luteolin, kaempferol, chrysoeriol, isorhamnetin, apigenin 7-O-glucoside, vitexin, kaempferol 3-O-glucoside, catechin, epicatechin, and quercitrin) were identified and quantified. The condensate exhibited higher TPC value and antioxidant activity than other wood industry effluents, positioning it as a promising natural antioxidant with potential applications in pharmaceutical and food industries. However, our short-term goal is to explore the potential use of WTSC as received - without isolating individual compounds - in studies focused on plant protection, textile dyeing, and wood-based panel production.",
journal = "Wood Science and Technology",
title = "Walnut wood steaming: chemical profile and antioxidant activity of the condensate to assess the potential application",
pages = "1628-1605",
number = "4",
volume = "58",
doi = "10.1007/s00226-024-01584-9",
url = "conv_1807"
}
Milić, G., Rančić, M., Todorović, N., Zivanović, N., Orcić, D.,& Simin, N.. (2024). Walnut wood steaming: chemical profile and antioxidant activity of the condensate to assess the potential application. in Wood Science and Technology, 58(4), 1605-1628.
https://doi.org/10.1007/s00226-024-01584-9
conv_1807
Milić G, Rančić M, Todorović N, Zivanović N, Orcić D, Simin N. Walnut wood steaming: chemical profile and antioxidant activity of the condensate to assess the potential application. in Wood Science and Technology. 2024;58(4):1605-1628.
doi:10.1007/s00226-024-01584-9
conv_1807 .
Milić, Goran, Rančić, Milica, Todorović, Nebojša, Zivanović, Nemanja, Orcić, Dejan, Simin, Natasa, "Walnut wood steaming: chemical profile and antioxidant activity of the condensate to assess the potential application" in Wood Science and Technology, 58, no. 4 (2024):1605-1628,
https://doi.org/10.1007/s00226-024-01584-9 .,
conv_1807 .
1
1
1

The effect of the beech wood steaming condensate on curing behaviour of urea-formaldehyde adhesive

Rančić, Milica; Popović, Mlađan; Milić, Goran; Todorović, Nebojša; Veizović, Marko; Gavrilović-Grmuša, Ivana

(2024)

TY  - JOUR
AU  - Rančić, Milica
AU  - Popović, Mlađan
AU  - Milić, Goran
AU  - Todorović, Nebojša
AU  - Veizović, Marko
AU  - Gavrilović-Grmuša, Ivana
PY  - 2024
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/1494
AB  - This study explores the potential of using condensate generated during beech wood steaming (BSC) as an eco-friendly additive in urea-formaldehyde (UF) adhesives for wood-based panel (WBP) production. The research aimed to assess the hardening behavior of pure commercial UF resin and UF with added condensate (UF-BSC), investigating the potential catalytic effect of BSC on the hardening characteristics of UF adhesives. Changes in chemical structure after the curing process were observed with Fourier transform infrared spectroscopy (FTIR). The curing kinetics was studied by differential scanning calorimetry (DSC) under a dynamic scanning regime with heating rates of 5, 10, and 20 degrees C/min. Obtained data were analyzed using Kissinger-Akahira-Sunose (KAS) and Friedman (FR) kinetic iso-conversional methods to estimate the activation energy (Ea) of the curing reaction in the investigated UF adhesive systems. The results of DSC analysis imply that BSC lowers the temperature of the curing reaction of UF adhesive along with the prolongation of the curing reaction. The obtained kinetic data supported by FTIR and chemical analysis suggest that phenolic compounds present in BSC interfere with the main curing reactions leading to lower peak temperatures but higher activation energy. & Tcy;his suggests that BSC increased the number of active sites involved in the reaction and, consequently, the number of collisions. BSC, as wastewater of the wood processing industry, can be efficiently utilized as an environmentally friendly, inexpensive substitute for deionized water in UF adhesive formulations for WBP manufacturing.
T2  - European Journal of Wood and Wood Products
T1  - The effect of the beech wood steaming condensate on curing behaviour of urea-formaldehyde adhesive
DO  - 10.1007/s00107-024-02151-6
UR  - conv_1827
ER  - 
@article{
author = "Rančić, Milica and Popović, Mlađan and Milić, Goran and Todorović, Nebojša and Veizović, Marko and Gavrilović-Grmuša, Ivana",
year = "2024",
abstract = "This study explores the potential of using condensate generated during beech wood steaming (BSC) as an eco-friendly additive in urea-formaldehyde (UF) adhesives for wood-based panel (WBP) production. The research aimed to assess the hardening behavior of pure commercial UF resin and UF with added condensate (UF-BSC), investigating the potential catalytic effect of BSC on the hardening characteristics of UF adhesives. Changes in chemical structure after the curing process were observed with Fourier transform infrared spectroscopy (FTIR). The curing kinetics was studied by differential scanning calorimetry (DSC) under a dynamic scanning regime with heating rates of 5, 10, and 20 degrees C/min. Obtained data were analyzed using Kissinger-Akahira-Sunose (KAS) and Friedman (FR) kinetic iso-conversional methods to estimate the activation energy (Ea) of the curing reaction in the investigated UF adhesive systems. The results of DSC analysis imply that BSC lowers the temperature of the curing reaction of UF adhesive along with the prolongation of the curing reaction. The obtained kinetic data supported by FTIR and chemical analysis suggest that phenolic compounds present in BSC interfere with the main curing reactions leading to lower peak temperatures but higher activation energy. & Tcy;his suggests that BSC increased the number of active sites involved in the reaction and, consequently, the number of collisions. BSC, as wastewater of the wood processing industry, can be efficiently utilized as an environmentally friendly, inexpensive substitute for deionized water in UF adhesive formulations for WBP manufacturing.",
journal = "European Journal of Wood and Wood Products",
title = "The effect of the beech wood steaming condensate on curing behaviour of urea-formaldehyde adhesive",
doi = "10.1007/s00107-024-02151-6",
url = "conv_1827"
}
Rančić, M., Popović, M., Milić, G., Todorović, N., Veizović, M.,& Gavrilović-Grmuša, I.. (2024). The effect of the beech wood steaming condensate on curing behaviour of urea-formaldehyde adhesive. in European Journal of Wood and Wood Products.
https://doi.org/10.1007/s00107-024-02151-6
conv_1827
Rančić M, Popović M, Milić G, Todorović N, Veizović M, Gavrilović-Grmuša I. The effect of the beech wood steaming condensate on curing behaviour of urea-formaldehyde adhesive. in European Journal of Wood and Wood Products. 2024;.
doi:10.1007/s00107-024-02151-6
conv_1827 .
Rančić, Milica, Popović, Mlađan, Milić, Goran, Todorović, Nebojša, Veizović, Marko, Gavrilović-Grmuša, Ivana, "The effect of the beech wood steaming condensate on curing behaviour of urea-formaldehyde adhesive" in European Journal of Wood and Wood Products (2024),
https://doi.org/10.1007/s00107-024-02151-6 .,
conv_1827 .

Heating Rate during Thermal Modification in Steam Atmosphere: Influence on the Properties of Maple and Ash Wood

Milić, Goran; Todorović, Nebojša; Veizović, Marko; Popadić, Ranko

(2023)

TY  - JOUR
AU  - Milić, Goran
AU  - Todorović, Nebojša
AU  - Veizović, Marko
AU  - Popadić, Ranko
PY  - 2023
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/1436
AB  - This study aimed to compare two thermal modification (TM) schedules-with short and long heating phases-and their influence on the properties of maple (Acer pseudoplatanus L.) and ash (Fraxinus excelsior L.) wood. Two TM runs were conducted in industrial conditions (open system, steam atmosphere; substantially longer method compared to the processes usually described in the literature), with the same peak phase (200 degrees C, 3 h), but with different heating rates-slow (1.1 degrees C/h) and fast (2.5 degrees C/h). The results revealed that both TMs significantly reduced hygroscopicity and swelling of wood, but the influence of slow heating rate-through prolonged exposure of wood to relatively high temperatures-on dimensional stability was more pronounced. The modulus of elasticity, compressive strength and Brinell hardness remained mostly unchanged after TM (except for fast-modified maple), while the modulus of rupture was strongly reduced by TM in both species. It is assumed-at least in the case of maple wood-that a combination of initial moisture content above 8% and fast heating rate during TM can cause more intensive degradation of wood polymers. Relatively small differences in colour between slow- and fast-modified wood were found. The results confirmed the hypothesis that the heating phase is an important part of the TM schedule, and it can directly affect (together with peak temperature and time) certain wood properties.
T2  - Forests
T1  - Heating Rate during Thermal Modification in Steam Atmosphere: Influence on the Properties of Maple and Ash Wood
IS  - 2
VL  - 14
DO  - 10.3390/f14020189
UR  - conv_1687
ER  - 
@article{
author = "Milić, Goran and Todorović, Nebojša and Veizović, Marko and Popadić, Ranko",
year = "2023",
abstract = "This study aimed to compare two thermal modification (TM) schedules-with short and long heating phases-and their influence on the properties of maple (Acer pseudoplatanus L.) and ash (Fraxinus excelsior L.) wood. Two TM runs were conducted in industrial conditions (open system, steam atmosphere; substantially longer method compared to the processes usually described in the literature), with the same peak phase (200 degrees C, 3 h), but with different heating rates-slow (1.1 degrees C/h) and fast (2.5 degrees C/h). The results revealed that both TMs significantly reduced hygroscopicity and swelling of wood, but the influence of slow heating rate-through prolonged exposure of wood to relatively high temperatures-on dimensional stability was more pronounced. The modulus of elasticity, compressive strength and Brinell hardness remained mostly unchanged after TM (except for fast-modified maple), while the modulus of rupture was strongly reduced by TM in both species. It is assumed-at least in the case of maple wood-that a combination of initial moisture content above 8% and fast heating rate during TM can cause more intensive degradation of wood polymers. Relatively small differences in colour between slow- and fast-modified wood were found. The results confirmed the hypothesis that the heating phase is an important part of the TM schedule, and it can directly affect (together with peak temperature and time) certain wood properties.",
journal = "Forests",
title = "Heating Rate during Thermal Modification in Steam Atmosphere: Influence on the Properties of Maple and Ash Wood",
number = "2",
volume = "14",
doi = "10.3390/f14020189",
url = "conv_1687"
}
Milić, G., Todorović, N., Veizović, M.,& Popadić, R.. (2023). Heating Rate during Thermal Modification in Steam Atmosphere: Influence on the Properties of Maple and Ash Wood. in Forests, 14(2).
https://doi.org/10.3390/f14020189
conv_1687
Milić G, Todorović N, Veizović M, Popadić R. Heating Rate during Thermal Modification in Steam Atmosphere: Influence on the Properties of Maple and Ash Wood. in Forests. 2023;14(2).
doi:10.3390/f14020189
conv_1687 .
Milić, Goran, Todorović, Nebojša, Veizović, Marko, Popadić, Ranko, "Heating Rate during Thermal Modification in Steam Atmosphere: Influence on the Properties of Maple and Ash Wood" in Forests, 14, no. 2 (2023),
https://doi.org/10.3390/f14020189 .,
conv_1687 .
2
2
2

Radijalna varijabilnost gustine drveta i dužine vlakana u drvetu crvenog hrasta (Quercus rubra L.)

Todorović, Nebojša; Živanović, Ivana; Vilotić, Dragica; Milić, Goran

(Institut za šumarstvo, Beograd, 2022)

TY  - JOUR
AU  - Todorović, Nebojša
AU  - Živanović, Ivana
AU  - Vilotić, Dragica
AU  - Milić, Goran
PY  - 2022
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/1373
AB  - Gustina drveta i dužina vlakana su dva svojstva drveta koje su od značaja za određivanje kvaliteta drveta za komercijalnu upotrebu. Dužina vlakana crvenog hrasta nije proučavana u istoj meri kao kod drugih vrsta hrasta. Cilj ovog rada je istraživanje anatomske varijacije i gustine drveta crvenog hrasta, kao dragocene informacije za istraživače u drugim oblastima izučavanja nauke o drvetu drveta. Uzorci su uzeti u sastojini crvenog hrasta starog 60 godina u južnom delu Beograda na lokalitetu Stepin Lug. Po južnom poluprečniku diska sečeni su uzorci 20 x 20 mm od beljike, zrelog i juvenilnog drveta. Gustina drveta u apsolutno suvom stanju vlažnosti i dužina vlakana merene su od srži do kore. Prema dobijenim podacima, prosečna gustina drveta iznosi 0,694 g/cm3. Najniža je u juvenilnom drvetu i kreće se od 0,628 do 0,681 g/cm3, zatim u delu beljike - 0,662 g/cm3, a najveća je u zrelom drvetu gde se gustina kreće od 0,707 do 0,740 g/cm3. Prikazane vrednosti pokazuju određene razlike, ali su i u skladu sa literaturnim podacima o gustini pojedinih industrijskih vrsta iz roda Quercus L. Dobijeni rezultati dužine drvnog vlakna pokazuju da ona varira od 0,99 do 1,33 mm koliko je izmerena kod zrelog drveta. Prosečna dužina u zreloj zoni je 1,26 (1,16-1,33) mm, dok je u juvenilnom području prosečna dužina 1,02 (0,85-1,23) mm. Na osnovu poznate dužine drvenih vlakana moguće je odrediti gustinu drveta crvenog hrasta. U ovom istraživanju utvrđen je pozitivan uticaj u oba dela stabla, juvenilnom i zrelom, ali je bolja matematička zavisnost dobijena u zoni zrelog drveta.
AB  - Wood density and fibre length are two wood properties that are important in determining the quality of wood for commercial use. The fibre length of red oak has not been studied to the same extent as in other oak species. The aim of this paper is to explore the anatomical variation and wood density of red oak wood, as valuable information for researchers in other fields. Samples were taken in a 60-year-old red oak stand in the south part of Belgrade on the site of Stepin Lug. Along the south radius, the disc samples of 20 x 20 mm were cut from the sapwood, mature and juvenile wood. Ovendry density and fibre length were measured from the pith to the bark. According to the obtained data, the average oven-dry density of wood per radius is 0.694 g/cm3 . The lowest is in the juvenile wood and ranges from 0.628 to 0.681 g/cm3 , then in the part of sapwood - 0.662 g/cm3 , and the highest is in the mature wood where the density ranges from 0.707 to 0.740 g/cm3 . The presented values show certain differences, but also conform to literature data on the density of some industrial species from the genus Quercus L. The obtained results of the wood fibre length show that it varies from 0.99 to 1.33 mm which was measured in mature wood. The average length in a mature zone is 1.26 (1.16-1.33) mm, while in a juvenile area the average length is 1.02 (0.85-1.23) mm. Based on the known wood fibre length, it is possible to determine the density of red oak wood. In this research, a positive influence was determined in both parts of the tree, juvenile and mature, but a better mathematical dependence was obtained in the mature zone.
PB  - Institut za šumarstvo, Beograd
T2  - Sustainable Forestry: Collection
T1  - Radijalna varijabilnost gustine drveta i dužine vlakana u drvetu crvenog hrasta (Quercus rubra L.)
T1  - Radial variability of wood density and fibre length in the red oak trees (Quercus rubra L.)
EP  - 86
IS  - 85-86
SP  - 75
DO  - 10.5937/SustFor2285075T
UR  - conv_772
ER  - 
@article{
author = "Todorović, Nebojša and Živanović, Ivana and Vilotić, Dragica and Milić, Goran",
year = "2022",
abstract = "Gustina drveta i dužina vlakana su dva svojstva drveta koje su od značaja za određivanje kvaliteta drveta za komercijalnu upotrebu. Dužina vlakana crvenog hrasta nije proučavana u istoj meri kao kod drugih vrsta hrasta. Cilj ovog rada je istraživanje anatomske varijacije i gustine drveta crvenog hrasta, kao dragocene informacije za istraživače u drugim oblastima izučavanja nauke o drvetu drveta. Uzorci su uzeti u sastojini crvenog hrasta starog 60 godina u južnom delu Beograda na lokalitetu Stepin Lug. Po južnom poluprečniku diska sečeni su uzorci 20 x 20 mm od beljike, zrelog i juvenilnog drveta. Gustina drveta u apsolutno suvom stanju vlažnosti i dužina vlakana merene su od srži do kore. Prema dobijenim podacima, prosečna gustina drveta iznosi 0,694 g/cm3. Najniža je u juvenilnom drvetu i kreće se od 0,628 do 0,681 g/cm3, zatim u delu beljike - 0,662 g/cm3, a najveća je u zrelom drvetu gde se gustina kreće od 0,707 do 0,740 g/cm3. Prikazane vrednosti pokazuju određene razlike, ali su i u skladu sa literaturnim podacima o gustini pojedinih industrijskih vrsta iz roda Quercus L. Dobijeni rezultati dužine drvnog vlakna pokazuju da ona varira od 0,99 do 1,33 mm koliko je izmerena kod zrelog drveta. Prosečna dužina u zreloj zoni je 1,26 (1,16-1,33) mm, dok je u juvenilnom području prosečna dužina 1,02 (0,85-1,23) mm. Na osnovu poznate dužine drvenih vlakana moguće je odrediti gustinu drveta crvenog hrasta. U ovom istraživanju utvrđen je pozitivan uticaj u oba dela stabla, juvenilnom i zrelom, ali je bolja matematička zavisnost dobijena u zoni zrelog drveta., Wood density and fibre length are two wood properties that are important in determining the quality of wood for commercial use. The fibre length of red oak has not been studied to the same extent as in other oak species. The aim of this paper is to explore the anatomical variation and wood density of red oak wood, as valuable information for researchers in other fields. Samples were taken in a 60-year-old red oak stand in the south part of Belgrade on the site of Stepin Lug. Along the south radius, the disc samples of 20 x 20 mm were cut from the sapwood, mature and juvenile wood. Ovendry density and fibre length were measured from the pith to the bark. According to the obtained data, the average oven-dry density of wood per radius is 0.694 g/cm3 . The lowest is in the juvenile wood and ranges from 0.628 to 0.681 g/cm3 , then in the part of sapwood - 0.662 g/cm3 , and the highest is in the mature wood where the density ranges from 0.707 to 0.740 g/cm3 . The presented values show certain differences, but also conform to literature data on the density of some industrial species from the genus Quercus L. The obtained results of the wood fibre length show that it varies from 0.99 to 1.33 mm which was measured in mature wood. The average length in a mature zone is 1.26 (1.16-1.33) mm, while in a juvenile area the average length is 1.02 (0.85-1.23) mm. Based on the known wood fibre length, it is possible to determine the density of red oak wood. In this research, a positive influence was determined in both parts of the tree, juvenile and mature, but a better mathematical dependence was obtained in the mature zone.",
publisher = "Institut za šumarstvo, Beograd",
journal = "Sustainable Forestry: Collection",
title = "Radijalna varijabilnost gustine drveta i dužine vlakana u drvetu crvenog hrasta (Quercus rubra L.), Radial variability of wood density and fibre length in the red oak trees (Quercus rubra L.)",
pages = "86-75",
number = "85-86",
doi = "10.5937/SustFor2285075T",
url = "conv_772"
}
Todorović, N., Živanović, I., Vilotić, D.,& Milić, G.. (2022). Radijalna varijabilnost gustine drveta i dužine vlakana u drvetu crvenog hrasta (Quercus rubra L.). in Sustainable Forestry: Collection
Institut za šumarstvo, Beograd.(85-86), 75-86.
https://doi.org/10.5937/SustFor2285075T
conv_772
Todorović N, Živanović I, Vilotić D, Milić G. Radijalna varijabilnost gustine drveta i dužine vlakana u drvetu crvenog hrasta (Quercus rubra L.). in Sustainable Forestry: Collection. 2022;(85-86):75-86.
doi:10.5937/SustFor2285075T
conv_772 .
Todorović, Nebojša, Živanović, Ivana, Vilotić, Dragica, Milić, Goran, "Radijalna varijabilnost gustine drveta i dužine vlakana u drvetu crvenog hrasta (Quercus rubra L.)" in Sustainable Forestry: Collection, no. 85-86 (2022):75-86,
https://doi.org/10.5937/SustFor2285075T .,
conv_772 .

Quality evaluation of heat-treated sessile oak ( Quercus petraea L.) wood by colour and FT-NIR spectroscopy

Todorović, Nebojša; Popović, Zdravko; Milić, Goran; Veizović, Marko; Popadić, Ranko

(2022)

TY  - JOUR
AU  - Todorović, Nebojša
AU  - Popović, Zdravko
AU  - Milić, Goran
AU  - Veizović, Marko
AU  - Popadić, Ranko
PY  - 2022
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/1355
AB  - The prediction of physical (wood density, mass loss) and mechanical (bending properties, compressive strength parallel to grain, and Brinell hardness) properties of heat-treated sessile oak (Quercus petraea L.) by FT-NIR spectroscopy, colour change, and partial least squares regression (PLS) was studied. Samples of oak sapwood and heartwood were treated for 4 h at temperatures at 170, 190, and 210 degrees C. FT-NIR spectra (100 scans and 4 cm(-1)) and colour parameters (CIE L*a*b* system) were collected on the radial surface before and after heat treatment. The applied heat treatment changed wood properties, darkened the colour and reduced the colour difference between heartwood and sapwood. According to the residual prediction deviation (RPD), most models obtained could be used for preliminary wood quality screening (1.5  lt  RPD  lt  2.0) and the properties of heartwood were better predicted than those of sapwood. Mass loss prediction by colour change can be used for quality control while for the other properties FT-NIR provided a more clear picture of the heat-treated oak wood and can serve as a quality indicator.
T2  - Wood Material Science & Engineering
T1  - Quality evaluation of heat-treated sessile oak ( Quercus petraea L.) wood by colour and FT-NIR spectroscopy
EP  - 209
IS  - 3
SP  - 202
VL  - 17
DO  - 10.1080/17480272.2020.1847188
UR  - conv_1510
ER  - 
@article{
author = "Todorović, Nebojša and Popović, Zdravko and Milić, Goran and Veizović, Marko and Popadić, Ranko",
year = "2022",
abstract = "The prediction of physical (wood density, mass loss) and mechanical (bending properties, compressive strength parallel to grain, and Brinell hardness) properties of heat-treated sessile oak (Quercus petraea L.) by FT-NIR spectroscopy, colour change, and partial least squares regression (PLS) was studied. Samples of oak sapwood and heartwood were treated for 4 h at temperatures at 170, 190, and 210 degrees C. FT-NIR spectra (100 scans and 4 cm(-1)) and colour parameters (CIE L*a*b* system) were collected on the radial surface before and after heat treatment. The applied heat treatment changed wood properties, darkened the colour and reduced the colour difference between heartwood and sapwood. According to the residual prediction deviation (RPD), most models obtained could be used for preliminary wood quality screening (1.5  lt  RPD  lt  2.0) and the properties of heartwood were better predicted than those of sapwood. Mass loss prediction by colour change can be used for quality control while for the other properties FT-NIR provided a more clear picture of the heat-treated oak wood and can serve as a quality indicator.",
journal = "Wood Material Science & Engineering",
title = "Quality evaluation of heat-treated sessile oak ( Quercus petraea L.) wood by colour and FT-NIR spectroscopy",
pages = "209-202",
number = "3",
volume = "17",
doi = "10.1080/17480272.2020.1847188",
url = "conv_1510"
}
Todorović, N., Popović, Z., Milić, G., Veizović, M.,& Popadić, R.. (2022). Quality evaluation of heat-treated sessile oak ( Quercus petraea L.) wood by colour and FT-NIR spectroscopy. in Wood Material Science & Engineering, 17(3), 202-209.
https://doi.org/10.1080/17480272.2020.1847188
conv_1510
Todorović N, Popović Z, Milić G, Veizović M, Popadić R. Quality evaluation of heat-treated sessile oak ( Quercus petraea L.) wood by colour and FT-NIR spectroscopy. in Wood Material Science & Engineering. 2022;17(3):202-209.
doi:10.1080/17480272.2020.1847188
conv_1510 .
Todorović, Nebojša, Popović, Zdravko, Milić, Goran, Veizović, Marko, Popadić, Ranko, "Quality evaluation of heat-treated sessile oak ( Quercus petraea L.) wood by colour and FT-NIR spectroscopy" in Wood Material Science & Engineering, 17, no. 3 (2022):202-209,
https://doi.org/10.1080/17480272.2020.1847188 .,
conv_1510 .
10
10
11

Svojstva drveta crvenog hrasta (Quercus rubra L.) određena fraktometrijskim merenjima - preliminarni rezultati

Živanović, Ivana; Jovanović, Filip; Šurjanac, Nenad; Todorović, Nebojša; Milić, Goran

(Univerzitet u Beogradu - Šumarski fakultet, Beograd, 2021)

TY  - JOUR
AU  - Živanović, Ivana
AU  - Jovanović, Filip
AU  - Šurjanac, Nenad
AU  - Todorović, Nebojša
AU  - Milić, Goran
PY  - 2021
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/1271
AB  - U ovom radu prikazani su preliminarni rezultati osnovnih svojstava drveta crvenog hrasta (Quercus rubra L.) kao i zavisnost između svojstava izvrtaka dobijenih na dubećem stablu i ispitivanih svojstava. Na stablu su izvađeni izvrtci prečnika 5 mm na kojima su, korišćenjem fraktometra, određeni: čvrstoća na pritisak paralelno sa vlakancima, radijalna čvrstoća na savijanje i ugao loma. Korišćenjem deskriptivne statistike i višestruke regresije utvrđena je zavisnost između fraktometrijskih parametara i osnovnih fizičko-mehaničkih svojstava drveta određenih destruktivnim metodama: gustine drveta, čvrstoće na pritisak paralelno sa vlakancima i savojnih svojstava (čvrstoća na savijanje i modul elastičnosti pri savijanju). Dobijene vrednosti ispitivanih svojstava crvenog hrasta se nalaze u granicama literaturnih podataka. Statistička analiza je pokazala da se radijalna čvrstoća na savijanje ne može koristiti kao pouzdan fraktometrijski parametar u proceni kvaliteta drveta. Sa druge strane, dobijeni rezultati sugerišu da se odnos između druga dva parametra (čvrstoće na pritisak paralelno sa vlakancima i ugla loma) i svojstava drveta crvenog hrasta može uspešno opisati korišćenjem modela višestruke regresione jednačine (koeficijent determinacije je bio u intervalu od 0,945 do 0,990).
AB  - This study presents preliminary results of the basic properties of the northern red oak wood as well as the relationship between the properties of the core samples obtained on the live tree and the tested properties. The core samples 5 mm in diameter were extracted from the tree and used for determining the fractometer properties: compressive strength parallel to grain, radial bending strength and braking angle. Using descriptive statistics and multiple regression, the relationship between fractometric parameters and basic physical and mechanical properties of wood determined by destructive methods (wood density, compressive strength in parallel with fibers and bending properties (bending strength and modulus of elasticity). The obtained values of the examined properties of northern red oak are within the limits of the literature data. Statistical analysis has shown that radial bending strength cannot be used as a reliable fractometric parameter in assessing wood quality. On the other hand, the obtained results suggest that the relationship between the other two parameters (compressive strength parallel to grain and fracture angle) and the properties of the northern red oak wood can be successfully described using the multiple regression models (coefficient of determination ranged from 0.945 to 0.990).
PB  - Univerzitet u Beogradu - Šumarski fakultet, Beograd
T2  - Glasnik Šumarskog fakulteta
T1  - Svojstva drveta crvenog hrasta (Quercus rubra L.) određena fraktometrijskim merenjima - preliminarni rezultati
T1  - Properties of the northern red oak (Quercus rubra L.) wood determined by fractometric mesurements: Preliminary results
EP  - 136
IS  - 124
SP  - 125
DO  - 10.2298/GSF2124125Z
UR  - conv_524
ER  - 
@article{
author = "Živanović, Ivana and Jovanović, Filip and Šurjanac, Nenad and Todorović, Nebojša and Milić, Goran",
year = "2021",
abstract = "U ovom radu prikazani su preliminarni rezultati osnovnih svojstava drveta crvenog hrasta (Quercus rubra L.) kao i zavisnost između svojstava izvrtaka dobijenih na dubećem stablu i ispitivanih svojstava. Na stablu su izvađeni izvrtci prečnika 5 mm na kojima su, korišćenjem fraktometra, određeni: čvrstoća na pritisak paralelno sa vlakancima, radijalna čvrstoća na savijanje i ugao loma. Korišćenjem deskriptivne statistike i višestruke regresije utvrđena je zavisnost između fraktometrijskih parametara i osnovnih fizičko-mehaničkih svojstava drveta određenih destruktivnim metodama: gustine drveta, čvrstoće na pritisak paralelno sa vlakancima i savojnih svojstava (čvrstoća na savijanje i modul elastičnosti pri savijanju). Dobijene vrednosti ispitivanih svojstava crvenog hrasta se nalaze u granicama literaturnih podataka. Statistička analiza je pokazala da se radijalna čvrstoća na savijanje ne može koristiti kao pouzdan fraktometrijski parametar u proceni kvaliteta drveta. Sa druge strane, dobijeni rezultati sugerišu da se odnos između druga dva parametra (čvrstoće na pritisak paralelno sa vlakancima i ugla loma) i svojstava drveta crvenog hrasta može uspešno opisati korišćenjem modela višestruke regresione jednačine (koeficijent determinacije je bio u intervalu od 0,945 do 0,990)., This study presents preliminary results of the basic properties of the northern red oak wood as well as the relationship between the properties of the core samples obtained on the live tree and the tested properties. The core samples 5 mm in diameter were extracted from the tree and used for determining the fractometer properties: compressive strength parallel to grain, radial bending strength and braking angle. Using descriptive statistics and multiple regression, the relationship between fractometric parameters and basic physical and mechanical properties of wood determined by destructive methods (wood density, compressive strength in parallel with fibers and bending properties (bending strength and modulus of elasticity). The obtained values of the examined properties of northern red oak are within the limits of the literature data. Statistical analysis has shown that radial bending strength cannot be used as a reliable fractometric parameter in assessing wood quality. On the other hand, the obtained results suggest that the relationship between the other two parameters (compressive strength parallel to grain and fracture angle) and the properties of the northern red oak wood can be successfully described using the multiple regression models (coefficient of determination ranged from 0.945 to 0.990).",
publisher = "Univerzitet u Beogradu - Šumarski fakultet, Beograd",
journal = "Glasnik Šumarskog fakulteta",
title = "Svojstva drveta crvenog hrasta (Quercus rubra L.) određena fraktometrijskim merenjima - preliminarni rezultati, Properties of the northern red oak (Quercus rubra L.) wood determined by fractometric mesurements: Preliminary results",
pages = "136-125",
number = "124",
doi = "10.2298/GSF2124125Z",
url = "conv_524"
}
Živanović, I., Jovanović, F., Šurjanac, N., Todorović, N.,& Milić, G.. (2021). Svojstva drveta crvenog hrasta (Quercus rubra L.) određena fraktometrijskim merenjima - preliminarni rezultati. in Glasnik Šumarskog fakulteta
Univerzitet u Beogradu - Šumarski fakultet, Beograd.(124), 125-136.
https://doi.org/10.2298/GSF2124125Z
conv_524
Živanović I, Jovanović F, Šurjanac N, Todorović N, Milić G. Svojstva drveta crvenog hrasta (Quercus rubra L.) određena fraktometrijskim merenjima - preliminarni rezultati. in Glasnik Šumarskog fakulteta. 2021;(124):125-136.
doi:10.2298/GSF2124125Z
conv_524 .
Živanović, Ivana, Jovanović, Filip, Šurjanac, Nenad, Todorović, Nebojša, Milić, Goran, "Svojstva drveta crvenog hrasta (Quercus rubra L.) određena fraktometrijskim merenjima - preliminarni rezultati" in Glasnik Šumarskog fakulteta, no. 124 (2021):125-136,
https://doi.org/10.2298/GSF2124125Z .,
conv_524 .

Promene vlažnosti elemenata bukve i jasena tokom dve godine izlaganja u sobnim uslovima

Milić, Goran

(Univerzitet u Beogradu - Šumarski fakultet, Beograd, 2021)

TY  - JOUR
AU  - Milić, Goran
PY  - 2021
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/1269
AB  - Predmet ovog rada je analiza promena vlažnosti drveta bukve i jasena tokom dve godine u sobnim uslovima (zimi grejanje, leti bez klimatizacije). Registrovane promene vlažnosti su prvenstveno rezultat promena relativne vlažnosti vazduha (merena je kapacitivnim sondama). Prosečne relativne vlažnosti vazduha u enterijeru su danas niže nego nekada što je pokazano i u ovom eksperimentu (prosečna relativna vlažnost vazduha tokom dve godine je iznosila 44%). Najnižu vlažnost je drvo dostizalo u vrlo hladnim zimskim danima kada je prostorija zagrevana i tokom noći - između 5% i 6%, a najvišu početkom juna: 10,4-10,9%. Očekivano, vlažnost drveta nije dostizala ravnotežnu vlažnost - tokom zime je vlažnost drveta za oko 1% viša, a leti niža i do 2,5% od ravnotežne. Potvrđena je preporuka da se rezana građa lišćara od koje će se izrađivati proizvodi za enterijer suši na 7-8% vlažnosti.
AB  - The subject of this paper is the analysis of moisture content (MC) changes of beech and ash wood during two years in room conditions (heating during winter; no air conditioning during summer). The registered MC changes are primarily the result of changes in relative humidity of the air (measured by capacitive probes). The average relative humidity of the air in the interior is lower today than in the past, as also shown in this experiment (the average relative humidity of air during two years was 44%). The lowest wood MC was reached on very cold winter days when the heating was on even during the night - between 5% and 6%, and the highest one at the beginning of June: 10.4-10.9%. As expected, the wood did not reach equilibrium moisture content - during winter, MC is by about 1% higher, and in summer it is lower by up to 2.5% than the equilibrium. The recommendation that the sawn timber from which the interior products will be made should be dried at 7-8% MC was confirmed.
PB  - Univerzitet u Beogradu - Šumarski fakultet, Beograd
T2  - Glasnik Šumarskog fakulteta
T1  - Promene vlažnosti elemenata bukve i jasena tokom dve godine izlaganja u sobnim uslovima
T1  - Moisture content changes of beech and ash elements during two years in room conditions
EP  - 110
IS  - 123
SP  - 97
DO  - 10.2298/GSF2123097M
UR  - conv_512
ER  - 
@article{
author = "Milić, Goran",
year = "2021",
abstract = "Predmet ovog rada je analiza promena vlažnosti drveta bukve i jasena tokom dve godine u sobnim uslovima (zimi grejanje, leti bez klimatizacije). Registrovane promene vlažnosti su prvenstveno rezultat promena relativne vlažnosti vazduha (merena je kapacitivnim sondama). Prosečne relativne vlažnosti vazduha u enterijeru su danas niže nego nekada što je pokazano i u ovom eksperimentu (prosečna relativna vlažnost vazduha tokom dve godine je iznosila 44%). Najnižu vlažnost je drvo dostizalo u vrlo hladnim zimskim danima kada je prostorija zagrevana i tokom noći - između 5% i 6%, a najvišu početkom juna: 10,4-10,9%. Očekivano, vlažnost drveta nije dostizala ravnotežnu vlažnost - tokom zime je vlažnost drveta za oko 1% viša, a leti niža i do 2,5% od ravnotežne. Potvrđena je preporuka da se rezana građa lišćara od koje će se izrađivati proizvodi za enterijer suši na 7-8% vlažnosti., The subject of this paper is the analysis of moisture content (MC) changes of beech and ash wood during two years in room conditions (heating during winter; no air conditioning during summer). The registered MC changes are primarily the result of changes in relative humidity of the air (measured by capacitive probes). The average relative humidity of the air in the interior is lower today than in the past, as also shown in this experiment (the average relative humidity of air during two years was 44%). The lowest wood MC was reached on very cold winter days when the heating was on even during the night - between 5% and 6%, and the highest one at the beginning of June: 10.4-10.9%. As expected, the wood did not reach equilibrium moisture content - during winter, MC is by about 1% higher, and in summer it is lower by up to 2.5% than the equilibrium. The recommendation that the sawn timber from which the interior products will be made should be dried at 7-8% MC was confirmed.",
publisher = "Univerzitet u Beogradu - Šumarski fakultet, Beograd",
journal = "Glasnik Šumarskog fakulteta",
title = "Promene vlažnosti elemenata bukve i jasena tokom dve godine izlaganja u sobnim uslovima, Moisture content changes of beech and ash elements during two years in room conditions",
pages = "110-97",
number = "123",
doi = "10.2298/GSF2123097M",
url = "conv_512"
}
Milić, G.. (2021). Promene vlažnosti elemenata bukve i jasena tokom dve godine izlaganja u sobnim uslovima. in Glasnik Šumarskog fakulteta
Univerzitet u Beogradu - Šumarski fakultet, Beograd.(123), 97-110.
https://doi.org/10.2298/GSF2123097M
conv_512
Milić G. Promene vlažnosti elemenata bukve i jasena tokom dve godine izlaganja u sobnim uslovima. in Glasnik Šumarskog fakulteta. 2021;(123):97-110.
doi:10.2298/GSF2123097M
conv_512 .
Milić, Goran, "Promene vlažnosti elemenata bukve i jasena tokom dve godine izlaganja u sobnim uslovima" in Glasnik Šumarskog fakulteta, no. 123 (2021):97-110,
https://doi.org/10.2298/GSF2123097M .,
conv_512 .

Sušenje hrastovih lamela - deo 1. analiza procesa u kondenzacionoj sušari

Milić, Goran; Todorović, Nebojša; Veizović, Marko; Popadić, Ranko

(Univerzitet u Beogradu - Šumarski fakultet, Beograd, 2021)

TY  - JOUR
AU  - Milić, Goran
AU  - Todorović, Nebojša
AU  - Veizović, Marko
AU  - Popadić, Ranko
PY  - 2021
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/1256
AB  - U radu je analizirana mogućnost sušenja hrastovih lamela - tankog sloja masivnog drveta u višeslojnom podu. Fokus prvog dela rada je na kondenzacionim sušarama koje su za sušenje hrastovih lamela alternativa konvencionalnim sušarama. Praćena su dva ciklusa sušenja u industrijskoj sušari i parametri sušenja poređeni sa arhivom ciklusa sušenja lamela u konvencionalnoj sušari. Istovremeno, sušenje lamela je sprovedeno u klima komori gde je primenjena viša početna temperatura. Pokazano je da se hrastove lamele debljine 5mm mogu uspešno sušiti u kondenzacionim sušarama, uz relativno kratko vreme sušenja i visok kvalitet. Sa primenjenim režimom (početna temperatura 36°C, konačna 46°C) očekivano je da ciklus sušenja traje od 2 do 5 dana, u zavisnosti od količine lamela i početne vlažnosti. Zbog velike brzine isparavanja vode i nemogućnosti sušare da je odstrane dovoljno brzo, sušenje lamela se i u kondenzacionim i u konvencionalnim sušarama odvija pri ravnotežnoj vlažnosti koja je viša od zadatih vrednosti.
AB  - The subject of this paper is to analyse the drying process of oak lamellas, which are the solid wood top layer of engineered wood flooring. The focus of the first part of the paper is on dehumidification kilns. Drying in a dehumidification kiln is an interesting alternative to conventional drying of thin solid oak wood with the aim of reaching high drying quality in a reasonable time. Drying tests were done in an industrial dehumidification kiln, and drying parameters were compared with the drying in the conventional kiln. Simultaneously, a drying test at a higher temperature was done in the programmable climate chamber. It was demonstrated that thin oak lamellas (approx. 5 mm thick) could be successfully dried in a dehumidification kiln in a relatively short time and with high drying quality. With the applied drying schedule (initial temperature of 36 °C, final temperature of 46 °C), the drying cycle will last 2 to 5 days, depending on the amount of wood and the initial MC. Due to the high rate of water evaporation and the inability of the kilns to remove it fast enough, the drying of lamellas in both dehumidification and conventional kilns takes place at a higher equilibrium moisture content than the set values.
PB  - Univerzitet u Beogradu - Šumarski fakultet, Beograd
T2  - Glasnik Šumarskog fakulteta
T1  - Sušenje hrastovih lamela - deo 1. analiza procesa u kondenzacionoj sušari
T1  - Drying of oak wood lamellas: Part 1. Analysis of the process in a dehumidification kiln
EP  - 58
IS  - 124
SP  - 45
DO  - 10.2298/GSF2124045M
UR  - conv_520
ER  - 
@article{
author = "Milić, Goran and Todorović, Nebojša and Veizović, Marko and Popadić, Ranko",
year = "2021",
abstract = "U radu je analizirana mogućnost sušenja hrastovih lamela - tankog sloja masivnog drveta u višeslojnom podu. Fokus prvog dela rada je na kondenzacionim sušarama koje su za sušenje hrastovih lamela alternativa konvencionalnim sušarama. Praćena su dva ciklusa sušenja u industrijskoj sušari i parametri sušenja poređeni sa arhivom ciklusa sušenja lamela u konvencionalnoj sušari. Istovremeno, sušenje lamela je sprovedeno u klima komori gde je primenjena viša početna temperatura. Pokazano je da se hrastove lamele debljine 5mm mogu uspešno sušiti u kondenzacionim sušarama, uz relativno kratko vreme sušenja i visok kvalitet. Sa primenjenim režimom (početna temperatura 36°C, konačna 46°C) očekivano je da ciklus sušenja traje od 2 do 5 dana, u zavisnosti od količine lamela i početne vlažnosti. Zbog velike brzine isparavanja vode i nemogućnosti sušare da je odstrane dovoljno brzo, sušenje lamela se i u kondenzacionim i u konvencionalnim sušarama odvija pri ravnotežnoj vlažnosti koja je viša od zadatih vrednosti., The subject of this paper is to analyse the drying process of oak lamellas, which are the solid wood top layer of engineered wood flooring. The focus of the first part of the paper is on dehumidification kilns. Drying in a dehumidification kiln is an interesting alternative to conventional drying of thin solid oak wood with the aim of reaching high drying quality in a reasonable time. Drying tests were done in an industrial dehumidification kiln, and drying parameters were compared with the drying in the conventional kiln. Simultaneously, a drying test at a higher temperature was done in the programmable climate chamber. It was demonstrated that thin oak lamellas (approx. 5 mm thick) could be successfully dried in a dehumidification kiln in a relatively short time and with high drying quality. With the applied drying schedule (initial temperature of 36 °C, final temperature of 46 °C), the drying cycle will last 2 to 5 days, depending on the amount of wood and the initial MC. Due to the high rate of water evaporation and the inability of the kilns to remove it fast enough, the drying of lamellas in both dehumidification and conventional kilns takes place at a higher equilibrium moisture content than the set values.",
publisher = "Univerzitet u Beogradu - Šumarski fakultet, Beograd",
journal = "Glasnik Šumarskog fakulteta",
title = "Sušenje hrastovih lamela - deo 1. analiza procesa u kondenzacionoj sušari, Drying of oak wood lamellas: Part 1. Analysis of the process in a dehumidification kiln",
pages = "58-45",
number = "124",
doi = "10.2298/GSF2124045M",
url = "conv_520"
}
Milić, G., Todorović, N., Veizović, M.,& Popadić, R.. (2021). Sušenje hrastovih lamela - deo 1. analiza procesa u kondenzacionoj sušari. in Glasnik Šumarskog fakulteta
Univerzitet u Beogradu - Šumarski fakultet, Beograd.(124), 45-58.
https://doi.org/10.2298/GSF2124045M
conv_520
Milić G, Todorović N, Veizović M, Popadić R. Sušenje hrastovih lamela - deo 1. analiza procesa u kondenzacionoj sušari. in Glasnik Šumarskog fakulteta. 2021;(124):45-58.
doi:10.2298/GSF2124045M
conv_520 .
Milić, Goran, Todorović, Nebojša, Veizović, Marko, Popadić, Ranko, "Sušenje hrastovih lamela - deo 1. analiza procesa u kondenzacionoj sušari" in Glasnik Šumarskog fakulteta, no. 124 (2021):45-58,
https://doi.org/10.2298/GSF2124045M .,
conv_520 .
2

Mogućnost sušenja elemenata hrasta i jasena sa korom

Milić, Goran; Veizović, Marko; Todorović, Nebojša

(Univerzitet u Beogradu - Šumarski fakultet, Beograd, 2020)

TY  - JOUR
AU  - Milić, Goran
AU  - Veizović, Marko
AU  - Todorović, Nebojša
PY  - 2020
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/1112
AB  - Predmet ovog rada je analiza mogućnosti sušenja rezanih elemenata hrasta i jasena sa prisutnom korom drveta na jednoj strani elementa. Osušena je jedna šarža hrastovih i jedna jasenovih elemenata pri čemu je proces vođen daljinskim elektrovlagomerima u sušari, ali je vlažnost određivana i gravimetrijskim metodom. Analizirane su i greške sušenja i njihovi uzroci. Rezultati su pokazali da se konvencionalno sušenje može koristiti za ovu namenu - trajanje je relativno kratko (do 7 dana), a varijacija konačne vlažnosti relativno mala. Osnovni problem je relativno veliki broj zakrivljenih elemenata na kraju sušenja, isključivo onih gde je učešće drveta u odnosu na koru malo. Vrlo visoki koeficijenti aksijalnog utezanja kore (4,5 puta veći od drveta) su uzrok ovih deformacija.
AB  - The subject of this paper is the analysis of the possibility of drying oak and ash elements with the presence of tree bark on one side of the element (bark edge). One batch was dried per species, and the process was controlled by moisture content (MC) probes in the kiln, but also determined by the oven-dry method. Drying defects and their causes were also analyzed. The results showed that conventional drying can be used for this purpose - the duration is relatively short (up to 7 days), and the variation of the final MC is relatively small. The main problem is a relatively large number of crooked elements at the end of drying, particularly those where the share of wood in relation to the bark was small. Very high axial shrinkage coefficients of the bark (4.5 times higher than wood) are the cause of these deformations.
PB  - Univerzitet u Beogradu - Šumarski fakultet, Beograd
T2  - Glasnik Šumarskog fakulteta
T1  - Mogućnost sušenja elemenata hrasta i jasena sa korom
T1  - Possibility of drying oak and ash elements with bark
EP  - 107
IS  - 121
SP  - 97
DO  - 10.2298/GSF2021097M
UR  - conv_500
ER  - 
@article{
author = "Milić, Goran and Veizović, Marko and Todorović, Nebojša",
year = "2020",
abstract = "Predmet ovog rada je analiza mogućnosti sušenja rezanih elemenata hrasta i jasena sa prisutnom korom drveta na jednoj strani elementa. Osušena je jedna šarža hrastovih i jedna jasenovih elemenata pri čemu je proces vođen daljinskim elektrovlagomerima u sušari, ali je vlažnost određivana i gravimetrijskim metodom. Analizirane su i greške sušenja i njihovi uzroci. Rezultati su pokazali da se konvencionalno sušenje može koristiti za ovu namenu - trajanje je relativno kratko (do 7 dana), a varijacija konačne vlažnosti relativno mala. Osnovni problem je relativno veliki broj zakrivljenih elemenata na kraju sušenja, isključivo onih gde je učešće drveta u odnosu na koru malo. Vrlo visoki koeficijenti aksijalnog utezanja kore (4,5 puta veći od drveta) su uzrok ovih deformacija., The subject of this paper is the analysis of the possibility of drying oak and ash elements with the presence of tree bark on one side of the element (bark edge). One batch was dried per species, and the process was controlled by moisture content (MC) probes in the kiln, but also determined by the oven-dry method. Drying defects and their causes were also analyzed. The results showed that conventional drying can be used for this purpose - the duration is relatively short (up to 7 days), and the variation of the final MC is relatively small. The main problem is a relatively large number of crooked elements at the end of drying, particularly those where the share of wood in relation to the bark was small. Very high axial shrinkage coefficients of the bark (4.5 times higher than wood) are the cause of these deformations.",
publisher = "Univerzitet u Beogradu - Šumarski fakultet, Beograd",
journal = "Glasnik Šumarskog fakulteta",
title = "Mogućnost sušenja elemenata hrasta i jasena sa korom, Possibility of drying oak and ash elements with bark",
pages = "107-97",
number = "121",
doi = "10.2298/GSF2021097M",
url = "conv_500"
}
Milić, G., Veizović, M.,& Todorović, N.. (2020). Mogućnost sušenja elemenata hrasta i jasena sa korom. in Glasnik Šumarskog fakulteta
Univerzitet u Beogradu - Šumarski fakultet, Beograd.(121), 97-107.
https://doi.org/10.2298/GSF2021097M
conv_500
Milić G, Veizović M, Todorović N. Mogućnost sušenja elemenata hrasta i jasena sa korom. in Glasnik Šumarskog fakulteta. 2020;(121):97-107.
doi:10.2298/GSF2021097M
conv_500 .
Milić, Goran, Veizović, Marko, Todorović, Nebojša, "Mogućnost sušenja elemenata hrasta i jasena sa korom" in Glasnik Šumarskog fakulteta, no. 121 (2020):97-107,
https://doi.org/10.2298/GSF2021097M .,
conv_500 .

Influence of climate oscillations on moisture content profiles of beech timber during initial stages of drying

Milić, Goran; Veizović, Marko; Todorović, Nebojša

(2020)

TY  - CONF
AU  - Milić, Goran
AU  - Veizović, Marko
AU  - Todorović, Nebojša
PY  - 2020
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/1119
AB  - This study aimed to determine the influence of equilibrium moisture content (EMC) oscillations on MC profiles of beech timber (38 x 120 x 500 mm) during drying in the climatic chamber. Two test runs with EMC oscillations (along with constant temperature) were followed by the equivalent test runs in constant climate: altogether, 4 drying runs were carried out. The amplitudes of EMC oscillations were ca. +/- 1.5% (absolute value) compared to the value in constant climate test, while the temperature in all cases was 35 degrees C. Among others, MC profile across thickness was periodically determined by slicing five lamellae and using the oven-dry method to determine their MC. Drying curves produced during constant and oscillation climate drying were similar and no statistical difference was found between average MC determined on the same day during constant and oscillation drying. In all cases it was found that MC difference between core and surface is lower (or at least not higher) in oscillating compared to constant climate conditions. This indicates that, if the positive influence of additional mechanosorptive creep (caused by EMC oscillations) on stresses in wood is taken into account, lower stresses in surface layers can be expected during oscillation drying. Further tests will be done to reveal the exact MC changes within surface layers of the boards. It is demonstrated that the climatic chamber is very stable in reaching and maintenance of air parameters during oscillation drying; it has practically no uncontrolled oscillations and will be used in further testing, along with the tests in semi-industrial and industrial kilns.
C3  - 9th Hardwood Proceedings, Vol 9 - Pt I: An Underutilized Resource: Hardwood Oriented Research
T1  - Influence of climate oscillations on moisture content profiles of beech timber during initial stages of drying
EP  - 199
SP  - 194
UR  - conv_1655
ER  - 
@conference{
author = "Milić, Goran and Veizović, Marko and Todorović, Nebojša",
year = "2020",
abstract = "This study aimed to determine the influence of equilibrium moisture content (EMC) oscillations on MC profiles of beech timber (38 x 120 x 500 mm) during drying in the climatic chamber. Two test runs with EMC oscillations (along with constant temperature) were followed by the equivalent test runs in constant climate: altogether, 4 drying runs were carried out. The amplitudes of EMC oscillations were ca. +/- 1.5% (absolute value) compared to the value in constant climate test, while the temperature in all cases was 35 degrees C. Among others, MC profile across thickness was periodically determined by slicing five lamellae and using the oven-dry method to determine their MC. Drying curves produced during constant and oscillation climate drying were similar and no statistical difference was found between average MC determined on the same day during constant and oscillation drying. In all cases it was found that MC difference between core and surface is lower (or at least not higher) in oscillating compared to constant climate conditions. This indicates that, if the positive influence of additional mechanosorptive creep (caused by EMC oscillations) on stresses in wood is taken into account, lower stresses in surface layers can be expected during oscillation drying. Further tests will be done to reveal the exact MC changes within surface layers of the boards. It is demonstrated that the climatic chamber is very stable in reaching and maintenance of air parameters during oscillation drying; it has practically no uncontrolled oscillations and will be used in further testing, along with the tests in semi-industrial and industrial kilns.",
journal = "9th Hardwood Proceedings, Vol 9 - Pt I: An Underutilized Resource: Hardwood Oriented Research",
title = "Influence of climate oscillations on moisture content profiles of beech timber during initial stages of drying",
pages = "199-194",
url = "conv_1655"
}
Milić, G., Veizović, M.,& Todorović, N.. (2020). Influence of climate oscillations on moisture content profiles of beech timber during initial stages of drying. in 9th Hardwood Proceedings, Vol 9 - Pt I: An Underutilized Resource: Hardwood Oriented Research, 194-199.
conv_1655
Milić G, Veizović M, Todorović N. Influence of climate oscillations on moisture content profiles of beech timber during initial stages of drying. in 9th Hardwood Proceedings, Vol 9 - Pt I: An Underutilized Resource: Hardwood Oriented Research. 2020;:194-199.
conv_1655 .
Milić, Goran, Veizović, Marko, Todorović, Nebojša, "Influence of climate oscillations on moisture content profiles of beech timber during initial stages of drying" in 9th Hardwood Proceedings, Vol 9 - Pt I: An Underutilized Resource: Hardwood Oriented Research (2020):194-199,
conv_1655 .

Influence of Diameter and Quality of Beech Logs on the Potential Energy of Sawmill Residues

Popadić, Ranko; Furtula, Mladen; Milić, Goran

(2019)

TY  - JOUR
AU  - Popadić, Ranko
AU  - Furtula, Mladen
AU  - Milić, Goran
PY  - 2019
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/1066
AB  - The influence of log diameter and log quality were studied relative to the potential heat energy produced from wood residue. Research was conducted on beech sawmill logs (30 cm to 49 cm in diameter and 4 m in length) of different qualities. Logs with greater diameters and of better quality increased the amount of products and decreased the amount of residue. A decrease in the diameter and quality of beech logs increased the total energy capacity, ranging between 840 kWh/m(3) (highest quality logs, 40 cm to 49 cm in diameter) and 1,350 kWh/m(3) (lower quality logs, 30 cm to 34 cm in diameter). Drying the lumber produced from logs of small diameters used less than 10% of the potential heating energy. However, logs of 40 cm to 49 cm in diameter increased this usage to 33%. When burner losses and drying energy losses were calculated, there was approximately 430 kWh/m(3) to 960 kWh/m(3) of leftover energy. This could be used for various purposes or it could be sold. The amount of obtained energy was influenced more by log diameter than by the log quality.
T2  - BioResources
T1  - Influence of Diameter and Quality of Beech Logs on the Potential Energy of Sawmill Residues
EP  - 6340
IS  - 3
SP  - 6331
VL  - 14
DO  - 10.15376/biores.14.3.6331-6340
UR  - conv_1437
ER  - 
@article{
author = "Popadić, Ranko and Furtula, Mladen and Milić, Goran",
year = "2019",
abstract = "The influence of log diameter and log quality were studied relative to the potential heat energy produced from wood residue. Research was conducted on beech sawmill logs (30 cm to 49 cm in diameter and 4 m in length) of different qualities. Logs with greater diameters and of better quality increased the amount of products and decreased the amount of residue. A decrease in the diameter and quality of beech logs increased the total energy capacity, ranging between 840 kWh/m(3) (highest quality logs, 40 cm to 49 cm in diameter) and 1,350 kWh/m(3) (lower quality logs, 30 cm to 34 cm in diameter). Drying the lumber produced from logs of small diameters used less than 10% of the potential heating energy. However, logs of 40 cm to 49 cm in diameter increased this usage to 33%. When burner losses and drying energy losses were calculated, there was approximately 430 kWh/m(3) to 960 kWh/m(3) of leftover energy. This could be used for various purposes or it could be sold. The amount of obtained energy was influenced more by log diameter than by the log quality.",
journal = "BioResources",
title = "Influence of Diameter and Quality of Beech Logs on the Potential Energy of Sawmill Residues",
pages = "6340-6331",
number = "3",
volume = "14",
doi = "10.15376/biores.14.3.6331-6340",
url = "conv_1437"
}
Popadić, R., Furtula, M.,& Milić, G.. (2019). Influence of Diameter and Quality of Beech Logs on the Potential Energy of Sawmill Residues. in BioResources, 14(3), 6331-6340.
https://doi.org/10.15376/biores.14.3.6331-6340
conv_1437
Popadić R, Furtula M, Milić G. Influence of Diameter and Quality of Beech Logs on the Potential Energy of Sawmill Residues. in BioResources. 2019;14(3):6331-6340.
doi:10.15376/biores.14.3.6331-6340
conv_1437 .
Popadić, Ranko, Furtula, Mladen, Milić, Goran, "Influence of Diameter and Quality of Beech Logs on the Potential Energy of Sawmill Residues" in BioResources, 14, no. 3 (2019):6331-6340,
https://doi.org/10.15376/biores.14.3.6331-6340 .,
conv_1437 .

Drying quality and colour of subfossil oak from central Serbia

Veizović, Marko; Popović, Zdravko; Todorović, Nebojša; Milić, Goran

(Univerzitet u Beogradu - Šumarski fakultet, Beograd, 2018)

TY  - JOUR
AU  - Veizović, Marko
AU  - Popović, Zdravko
AU  - Todorović, Nebojša
AU  - Milić, Goran
PY  - 2018
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/935
AB  - The subject of this paper is the analysis of the quality of natural and
   conventional drying of subfossil oak wood. In addition to the drying
   quality, the colour of this material, as well as the effect of the drying
   process on colour change have been tested. The subfossil oak logs that were
   used in this experiment originate from the Morava River in Central Serbia.
   After sawing, timber was air-dried to about 20% moisture content (MC)
   followed by kiln-drying to 9.5% MC. By examining the quality of air-drying
   of the subfossil oak wood, a high presence of cracks was found, as well as
   the inaccuracy of humidity measurement using electric moisture meters. The
   stack for kiln-drying consisted of 24 boards, of which 4 were used for the
   monitoring of MC and MC distribution across the thickness of plank during
   drying. Drying quality was evaluated after the kiln-drying process. Although
   mild drying conditions during kiln-drying were applied, the gap as a measure
   of case-hardening had a value greater than usual for oak of same thickness.
   It was found that the drying process has no significant effect on the change
   in the colour of subfossil wood. The colour of the subfossil oak wood was
   significantly darker than the usual oak wood, and the colour difference
   between the central and the outer parts of the trunk of the subfossil oak
   was determined.
PB  - Univerzitet u Beogradu - Šumarski fakultet, Beograd
T2  - Glasnik Šumarskog Fakulteta: Univerzitet u Beogradu
T1  - Drying quality and colour of subfossil oak from central Serbia
EP  - 172
IS  - 117
SP  - 157
VL  - 2018
DO  - 10.2298/GSF1817157V
UR  - conv_2370
ER  - 
@article{
author = "Veizović, Marko and Popović, Zdravko and Todorović, Nebojša and Milić, Goran",
year = "2018",
abstract = "The subject of this paper is the analysis of the quality of natural and
   conventional drying of subfossil oak wood. In addition to the drying
   quality, the colour of this material, as well as the effect of the drying
   process on colour change have been tested. The subfossil oak logs that were
   used in this experiment originate from the Morava River in Central Serbia.
   After sawing, timber was air-dried to about 20% moisture content (MC)
   followed by kiln-drying to 9.5% MC. By examining the quality of air-drying
   of the subfossil oak wood, a high presence of cracks was found, as well as
   the inaccuracy of humidity measurement using electric moisture meters. The
   stack for kiln-drying consisted of 24 boards, of which 4 were used for the
   monitoring of MC and MC distribution across the thickness of plank during
   drying. Drying quality was evaluated after the kiln-drying process. Although
   mild drying conditions during kiln-drying were applied, the gap as a measure
   of case-hardening had a value greater than usual for oak of same thickness.
   It was found that the drying process has no significant effect on the change
   in the colour of subfossil wood. The colour of the subfossil oak wood was
   significantly darker than the usual oak wood, and the colour difference
   between the central and the outer parts of the trunk of the subfossil oak
   was determined.",
publisher = "Univerzitet u Beogradu - Šumarski fakultet, Beograd",
journal = "Glasnik Šumarskog Fakulteta: Univerzitet u Beogradu",
title = "Drying quality and colour of subfossil oak from central Serbia",
pages = "172-157",
number = "117",
volume = "2018",
doi = "10.2298/GSF1817157V",
url = "conv_2370"
}
Veizović, M., Popović, Z., Todorović, N.,& Milić, G.. (2018). Drying quality and colour of subfossil oak from central Serbia. in Glasnik Šumarskog Fakulteta: Univerzitet u Beogradu
Univerzitet u Beogradu - Šumarski fakultet, Beograd., 2018(117), 157-172.
https://doi.org/10.2298/GSF1817157V
conv_2370
Veizović M, Popović Z, Todorović N, Milić G. Drying quality and colour of subfossil oak from central Serbia. in Glasnik Šumarskog Fakulteta: Univerzitet u Beogradu. 2018;2018(117):157-172.
doi:10.2298/GSF1817157V
conv_2370 .
Veizović, Marko, Popović, Zdravko, Todorović, Nebojša, Milić, Goran, "Drying quality and colour of subfossil oak from central Serbia" in Glasnik Šumarskog Fakulteta: Univerzitet u Beogradu, 2018, no. 117 (2018):157-172,
https://doi.org/10.2298/GSF1817157V .,
conv_2370 .
3

Properties of less valuable parts of beech and sessile oak wood after thermal modification

Todorović, Nebojša; Popović, Zdravko; Milić, Goran; Veizović, Marko

(2018)

TY  - CONF
AU  - Todorović, Nebojša
AU  - Popović, Zdravko
AU  - Milić, Goran
AU  - Veizović, Marko
PY  - 2018
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/957
C3  - 8th Hardwood Conference With Special Focus on New Aspects on Hardwood Utilization - From Science To Technology
T1  - Properties of less valuable parts of beech and sessile oak wood after thermal modification
EP  - 122
SP  - 121
UR  - conv_1439
ER  - 
@conference{
author = "Todorović, Nebojša and Popović, Zdravko and Milić, Goran and Veizović, Marko",
year = "2018",
journal = "8th Hardwood Conference With Special Focus on New Aspects on Hardwood Utilization - From Science To Technology",
title = "Properties of less valuable parts of beech and sessile oak wood after thermal modification",
pages = "122-121",
url = "conv_1439"
}
Todorović, N., Popović, Z., Milić, G.,& Veizović, M.. (2018). Properties of less valuable parts of beech and sessile oak wood after thermal modification. in 8th Hardwood Conference With Special Focus on New Aspects on Hardwood Utilization - From Science To Technology, 121-122.
conv_1439
Todorović N, Popović Z, Milić G, Veizović M. Properties of less valuable parts of beech and sessile oak wood after thermal modification. in 8th Hardwood Conference With Special Focus on New Aspects on Hardwood Utilization - From Science To Technology. 2018;:121-122.
conv_1439 .
Todorović, Nebojša, Popović, Zdravko, Milić, Goran, Veizović, Marko, "Properties of less valuable parts of beech and sessile oak wood after thermal modification" in 8th Hardwood Conference With Special Focus on New Aspects on Hardwood Utilization - From Science To Technology (2018):121-122,
conv_1439 .

Properties of Plywood Boards Composed of Thermally Modified and Non-modified Poplar Veneer

Lovrić, Aleksandar; Zdravković, Vladislav; Popadić, Ranko; Milić, Goran

(2017)

TY  - JOUR
AU  - Lovrić, Aleksandar
AU  - Zdravković, Vladislav
AU  - Popadić, Ranko
AU  - Milić, Goran
PY  - 2017
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/877
AB  - Possibilities for use of thermally modified poplar veneer were evaluated for the production of plywood boards in industrial conditions. Formats of poplar veneer were treated at temperatures of 190 degrees C, 200 degrees C, 210 degrees C, and 215 degrees C for 1 h. By combining the treated and non-treated formats of veneer, thirteen different types of board were made. Analyses showed that the examined physical and mechanical properties were influenced by both the type of construction and the applied thermal treatment. Boards composed only of thermally modified veneer achieved the best results regarding moisture absorption and dimensional stability, and boards composed of the combined veneers had better mechanical properties. Treatments at 200 degrees C and 210 degrees C proved to be optimal, while the treatment at 215 degrees C was too harsh and should not be used for the thermal modification of poplar veneer.
T2  - BioResources
T1  - Properties of Plywood Boards Composed of Thermally Modified and Non-modified Poplar Veneer
EP  - 8594
IS  - 4
SP  - 8581
VL  - 12
DO  - 10.15376/biores.12.4.8581-8594
UR  - conv_1321
ER  - 
@article{
author = "Lovrić, Aleksandar and Zdravković, Vladislav and Popadić, Ranko and Milić, Goran",
year = "2017",
abstract = "Possibilities for use of thermally modified poplar veneer were evaluated for the production of plywood boards in industrial conditions. Formats of poplar veneer were treated at temperatures of 190 degrees C, 200 degrees C, 210 degrees C, and 215 degrees C for 1 h. By combining the treated and non-treated formats of veneer, thirteen different types of board were made. Analyses showed that the examined physical and mechanical properties were influenced by both the type of construction and the applied thermal treatment. Boards composed only of thermally modified veneer achieved the best results regarding moisture absorption and dimensional stability, and boards composed of the combined veneers had better mechanical properties. Treatments at 200 degrees C and 210 degrees C proved to be optimal, while the treatment at 215 degrees C was too harsh and should not be used for the thermal modification of poplar veneer.",
journal = "BioResources",
title = "Properties of Plywood Boards Composed of Thermally Modified and Non-modified Poplar Veneer",
pages = "8594-8581",
number = "4",
volume = "12",
doi = "10.15376/biores.12.4.8581-8594",
url = "conv_1321"
}
Lovrić, A., Zdravković, V., Popadić, R.,& Milić, G.. (2017). Properties of Plywood Boards Composed of Thermally Modified and Non-modified Poplar Veneer. in BioResources, 12(4), 8581-8594.
https://doi.org/10.15376/biores.12.4.8581-8594
conv_1321
Lovrić A, Zdravković V, Popadić R, Milić G. Properties of Plywood Boards Composed of Thermally Modified and Non-modified Poplar Veneer. in BioResources. 2017;12(4):8581-8594.
doi:10.15376/biores.12.4.8581-8594
conv_1321 .
Lovrić, Aleksandar, Zdravković, Vladislav, Popadić, Ranko, Milić, Goran, "Properties of Plywood Boards Composed of Thermally Modified and Non-modified Poplar Veneer" in BioResources, 12, no. 4 (2017):8581-8594,
https://doi.org/10.15376/biores.12.4.8581-8594 .,
conv_1321 .
8
9
12

Analiza mehanosorpcionog efekta pri oscilatornom sušenju rezane građe bukve

Milić, Goran; Todorović, Nebojša

(Univerzitet u Beogradu - Šumarski fakultet, Beograd, 2016)

TY  - JOUR
AU  - Milić, Goran
AU  - Todorović, Nebojša
PY  - 2016
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/767
AB  - U radu su prikazani rezultati analize uticaja oscilirajućih parametara sušenja na merenje vlažnosti drveta u sušari, brzinu i kvalitet sušenja. Za analizu su korišćeni konvencionalni ciklus sušenja, ciklus sa oscilacijama ravnotežne vlažnosti i ciklus sa oscilacijama temperature. Za zadavanje i ostvarenje oscilacija kreiran je poseban softverski dodatak. Pokazano je da oscilacije i ravnotežne vlažnosti i temperature dovode do cikličnih promena vlažnosti drveta, ali i do dodatne nepreciznosti merenja vlažnosti u sušari. Sušenje šarže sa oscilacijama ravnotežne vlažnosti je trajalo nešto kraće u odnosu na druge dve šarže. Kvalitet sušenja je bio isti ili bolji u šaržama sa oscilacijama u odnosu na konvencionalnu šaržu, a manja naprezanja u drvetu su potvrdila aktiviranje dodatnog mehanosorpcionog efekta tokom cikličnih promena vlažnosti u površinskim slojevima.
AB  - The paper shows results of analysis of influences of oscillating parameters of drying on measuring wood moisture content in the kiln, rate and quality of drying. For this analysis, we used a conventional drying cycle, a cycle with oscillating equilibrium moisture content (EMC), and a cycle with oscillating temperatures. A special software tool was created for managing the oscillations. It was shown that oscillations of EMC and temperatures result in cyclic changes in wood MC, but also in the additional inaccuracies of MC measurements in the kiln. The drying process of the cycle with oscillating EMC lasted somewhat shorter than the other two cycles. Drying quality was the same or better in the cycles with oscillations as compared to the conventionally dried cycle, and the smaller tensions in the wood confirmed the activation of the additional mechano-sorptive effect during cyclic changes of MC in surface layers.
PB  - Univerzitet u Beogradu - Šumarski fakultet, Beograd
T2  - Glasnik Šumarskog fakulteta
T1  - Analiza mehanosorpcionog efekta pri oscilatornom sušenju rezane građe bukve
T1  - Analysis of mechano-sorptive effect in oscillatory drying of beech timber
EP  - 136
IS  - 114
SP  - 119
DO  - 10.2298/GSF1614119M
UR  - conv_445
ER  - 
@article{
author = "Milić, Goran and Todorović, Nebojša",
year = "2016",
abstract = "U radu su prikazani rezultati analize uticaja oscilirajućih parametara sušenja na merenje vlažnosti drveta u sušari, brzinu i kvalitet sušenja. Za analizu su korišćeni konvencionalni ciklus sušenja, ciklus sa oscilacijama ravnotežne vlažnosti i ciklus sa oscilacijama temperature. Za zadavanje i ostvarenje oscilacija kreiran je poseban softverski dodatak. Pokazano je da oscilacije i ravnotežne vlažnosti i temperature dovode do cikličnih promena vlažnosti drveta, ali i do dodatne nepreciznosti merenja vlažnosti u sušari. Sušenje šarže sa oscilacijama ravnotežne vlažnosti je trajalo nešto kraće u odnosu na druge dve šarže. Kvalitet sušenja je bio isti ili bolji u šaržama sa oscilacijama u odnosu na konvencionalnu šaržu, a manja naprezanja u drvetu su potvrdila aktiviranje dodatnog mehanosorpcionog efekta tokom cikličnih promena vlažnosti u površinskim slojevima., The paper shows results of analysis of influences of oscillating parameters of drying on measuring wood moisture content in the kiln, rate and quality of drying. For this analysis, we used a conventional drying cycle, a cycle with oscillating equilibrium moisture content (EMC), and a cycle with oscillating temperatures. A special software tool was created for managing the oscillations. It was shown that oscillations of EMC and temperatures result in cyclic changes in wood MC, but also in the additional inaccuracies of MC measurements in the kiln. The drying process of the cycle with oscillating EMC lasted somewhat shorter than the other two cycles. Drying quality was the same or better in the cycles with oscillations as compared to the conventionally dried cycle, and the smaller tensions in the wood confirmed the activation of the additional mechano-sorptive effect during cyclic changes of MC in surface layers.",
publisher = "Univerzitet u Beogradu - Šumarski fakultet, Beograd",
journal = "Glasnik Šumarskog fakulteta",
title = "Analiza mehanosorpcionog efekta pri oscilatornom sušenju rezane građe bukve, Analysis of mechano-sorptive effect in oscillatory drying of beech timber",
pages = "136-119",
number = "114",
doi = "10.2298/GSF1614119M",
url = "conv_445"
}
Milić, G.,& Todorović, N.. (2016). Analiza mehanosorpcionog efekta pri oscilatornom sušenju rezane građe bukve. in Glasnik Šumarskog fakulteta
Univerzitet u Beogradu - Šumarski fakultet, Beograd.(114), 119-136.
https://doi.org/10.2298/GSF1614119M
conv_445
Milić G, Todorović N. Analiza mehanosorpcionog efekta pri oscilatornom sušenju rezane građe bukve. in Glasnik Šumarskog fakulteta. 2016;(114):119-136.
doi:10.2298/GSF1614119M
conv_445 .
Milić, Goran, Todorović, Nebojša, "Analiza mehanosorpcionog efekta pri oscilatornom sušenju rezane građe bukve" in Glasnik Šumarskog fakulteta, no. 114 (2016):119-136,
https://doi.org/10.2298/GSF1614119M .,
conv_445 .

Uticaj termičkog tretmana na promenu boje bukovog drveta sa lažnom srčevinom

Todorović, Nebojša; Popović, Zdravko; Milić, Goran; Popadić, Ranko

(Univerzitet u Beogradu - Šumarski fakultet, Beograd, 2016)

TY  - JOUR
AU  - Todorović, Nebojša
AU  - Popović, Zdravko
AU  - Milić, Goran
AU  - Popadić, Ranko
PY  - 2016
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/762
AB  - Cilj ovog rada je bio da se istraže parametri boje bukovog drveta pre i posle termičkog tretmana, kao i da se odredi da li postoji razlika u boji između beljike i lažne srčevine pre i posle primene visoke temperature. Uzorci su tretirani na temperaturama od 170°C, 190°C odnosno 210°C, u trajanju od 4 h. Koordinate boje (CIEL*a*b*sistem), su izmerene pre i posle tretmana pri čemu su određeni sledeći parametri: ΔL, Δa, Δb i ΔE - promena boje. Boja je izmerena na 4 mesta na radijalnoj i poprečnoj površini drveta i uzeta je njihova prosečna vrednost za dalje istraživanje. Dobijeni rezultati pokazuju da primenjen termički tretman beljike nije značajno uticao na promenu razlike u boji između poprečne i radijalne površine. Razlika između poprečne i radijalne površine, kod netretirane lažne srčevine, je manja od vrednosti izmerene kod beljike. Razlika u boji netretirane beljike i lažne srčevine je više izražena na radijalnoj nego na poprečnoj površini. Dejstvom visoke temperature dolazi do značajnog smanjenja ove razlike. Temperatura od 210°C je proizvela najmanju razliku u boji između ova dva dela drveta koja je u ovom istraživanju utvrđena na radijalnoj površini. Zaključak je da primenjen termički tretman dovodi do približno iste boje beljike i lažne srčevine, pogotovu na radijalnoj površini, i sa tog stanovišta se može zaključiti da su ova dva dela bukovog drveta u tom smislu potpuno izjednačena. Pri ovoj konstataciji ne treba izostaviti ni pretpostavku da se u slučaju izjednačenih svostava, beljika i lažna srčevina mogu jednako upotrebiti u gotovom proizvodu od termički tretiranog bukovog drveta.
AB  - The goal of this word was to examine the parameters of color of beech wood before and after thermal treatment, and to determine if there is a difference in color between sapwood and red heartwood before and after application of high temperature. Samples were treated at temperatures of 170°C, 190°C and 210°C, respectively, during 4 hours. Color coordinates (CIEL*a*b*system) were measured before and after treatment by using the following parameters: ΔL, Δa, Δb and ΔE - color change. Color was assessed at four spots on the radial and cross-section surfaces of wood and their mean values were taken for further calculations. Acquired results show that the applied heat treatment of sapwood did not significantly influence the change of color difference between cross-section and radial surfaces. The difference between cross-section and radial surfaces, in nontreated red heartwood was smaller than that measured in sapwood. The color difference of nontreated sapwood and red heartwood was more pronounced on the radial than on the cross-section surface. Application of high temperature caused a significant decrease of this difference. Temperature of 210°C caused the smallest color difference between these two parts of wood which was in this research determined on the radial surface. It was concluded that the applied thermal treatment almost equalized the colors of sapwood and red heartwood, especially on the radial surface, and from this aspect it can be concluded that these two parts of beech wood were completely equalized. It should also be noted that in the case of equalized properties, sapwood and red heartwood can be equally applied in a final product made of thermally treated beech wood.
PB  - Univerzitet u Beogradu - Šumarski fakultet, Beograd
T2  - Glasnik Šumarskog fakulteta
T1  - Uticaj termičkog tretmana na promenu boje bukovog drveta sa lažnom srčevinom
T1  - Influence of thermal treatment on color change of beech wood with red heartwood
EP  - 256
IS  - 114
SP  - 239
DO  - 10.2298/GSF1614239T
UR  - conv_450
ER  - 
@article{
author = "Todorović, Nebojša and Popović, Zdravko and Milić, Goran and Popadić, Ranko",
year = "2016",
abstract = "Cilj ovog rada je bio da se istraže parametri boje bukovog drveta pre i posle termičkog tretmana, kao i da se odredi da li postoji razlika u boji između beljike i lažne srčevine pre i posle primene visoke temperature. Uzorci su tretirani na temperaturama od 170°C, 190°C odnosno 210°C, u trajanju od 4 h. Koordinate boje (CIEL*a*b*sistem), su izmerene pre i posle tretmana pri čemu su određeni sledeći parametri: ΔL, Δa, Δb i ΔE - promena boje. Boja je izmerena na 4 mesta na radijalnoj i poprečnoj površini drveta i uzeta je njihova prosečna vrednost za dalje istraživanje. Dobijeni rezultati pokazuju da primenjen termički tretman beljike nije značajno uticao na promenu razlike u boji između poprečne i radijalne površine. Razlika između poprečne i radijalne površine, kod netretirane lažne srčevine, je manja od vrednosti izmerene kod beljike. Razlika u boji netretirane beljike i lažne srčevine je više izražena na radijalnoj nego na poprečnoj površini. Dejstvom visoke temperature dolazi do značajnog smanjenja ove razlike. Temperatura od 210°C je proizvela najmanju razliku u boji između ova dva dela drveta koja je u ovom istraživanju utvrđena na radijalnoj površini. Zaključak je da primenjen termički tretman dovodi do približno iste boje beljike i lažne srčevine, pogotovu na radijalnoj površini, i sa tog stanovišta se može zaključiti da su ova dva dela bukovog drveta u tom smislu potpuno izjednačena. Pri ovoj konstataciji ne treba izostaviti ni pretpostavku da se u slučaju izjednačenih svostava, beljika i lažna srčevina mogu jednako upotrebiti u gotovom proizvodu od termički tretiranog bukovog drveta., The goal of this word was to examine the parameters of color of beech wood before and after thermal treatment, and to determine if there is a difference in color between sapwood and red heartwood before and after application of high temperature. Samples were treated at temperatures of 170°C, 190°C and 210°C, respectively, during 4 hours. Color coordinates (CIEL*a*b*system) were measured before and after treatment by using the following parameters: ΔL, Δa, Δb and ΔE - color change. Color was assessed at four spots on the radial and cross-section surfaces of wood and their mean values were taken for further calculations. Acquired results show that the applied heat treatment of sapwood did not significantly influence the change of color difference between cross-section and radial surfaces. The difference between cross-section and radial surfaces, in nontreated red heartwood was smaller than that measured in sapwood. The color difference of nontreated sapwood and red heartwood was more pronounced on the radial than on the cross-section surface. Application of high temperature caused a significant decrease of this difference. Temperature of 210°C caused the smallest color difference between these two parts of wood which was in this research determined on the radial surface. It was concluded that the applied thermal treatment almost equalized the colors of sapwood and red heartwood, especially on the radial surface, and from this aspect it can be concluded that these two parts of beech wood were completely equalized. It should also be noted that in the case of equalized properties, sapwood and red heartwood can be equally applied in a final product made of thermally treated beech wood.",
publisher = "Univerzitet u Beogradu - Šumarski fakultet, Beograd",
journal = "Glasnik Šumarskog fakulteta",
title = "Uticaj termičkog tretmana na promenu boje bukovog drveta sa lažnom srčevinom, Influence of thermal treatment on color change of beech wood with red heartwood",
pages = "256-239",
number = "114",
doi = "10.2298/GSF1614239T",
url = "conv_450"
}
Todorović, N., Popović, Z., Milić, G.,& Popadić, R.. (2016). Uticaj termičkog tretmana na promenu boje bukovog drveta sa lažnom srčevinom. in Glasnik Šumarskog fakulteta
Univerzitet u Beogradu - Šumarski fakultet, Beograd.(114), 239-256.
https://doi.org/10.2298/GSF1614239T
conv_450
Todorović N, Popović Z, Milić G, Popadić R. Uticaj termičkog tretmana na promenu boje bukovog drveta sa lažnom srčevinom. in Glasnik Šumarskog fakulteta. 2016;(114):239-256.
doi:10.2298/GSF1614239T
conv_450 .
Todorović, Nebojša, Popović, Zdravko, Milić, Goran, Popadić, Ranko, "Uticaj termičkog tretmana na promenu boje bukovog drveta sa lažnom srčevinom" in Glasnik Šumarskog fakulteta, no. 114 (2016):239-256,
https://doi.org/10.2298/GSF1614239T .,
conv_450 .

Uticaj parenja na kvalitet sušenja i boju rezane građe bukve

Milić, Goran; Todorović, Nebojša; Popadić, Ranko

(Univerzitet u Beogradu - Šumarski fakultet, Beograd, 2015)

TY  - JOUR
AU  - Milić, Goran
AU  - Todorović, Nebojša
AU  - Popadić, Ranko
PY  - 2015
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/670
AB  - U radu su prikazani rezultati analize uticaja tzv. blagog parenja na konvencionalno sušenje i boju tako osušene rezane građe bukve. Osušena je šarža koja se sastojala od parenih i neparenih dasaka. Praćeni su vlažnost i profili vlažnosti tokom sušenja, a na kraju sušenja su određivani konačna vlažnost, razlika vlažnosti po debljini građe, skorelost i boja. Statistički značajna razlika između parene i neparene građe nije utvrđena ni kod jednog ispitivanog parametra. Rezultati pokazuju da se može očekivati isti (ili čak bolji) kvalitet sušenja parene bukove građe u odnosu na neparenu sušenu istim režimom. Osušena parena rezana građa je imala tamniju boju sa većim učešćem crvene u odnosu na neparenu građu. Utvrđena je nepreciznost merenja vlažnosti parenog i neparenog drveta bukve u sušari u području vlažnosti 7-15% i data preporuka za prevazilaženje ovog problema.
AB  - This paper presents the results of an analysis of influence of the 'light' steaming process on conventional drying and colour of beech timber. A stack consisting of steamed and unsteamed boards was dried. Moisture content and moisture content profiles were recorded, and at the end of drying final moisture content, moisture content difference across thickness, case-hardening and colour were determinated. No statistically significant difference between steamed and unsteamed timber was established in any of the examined parameters (MC, ΔMC, gap). The results indicate that equal (or even) better drying quality can be expected with steamed beech timber than with unsteamed timber, given the same drying schedule. Dry steamed timber was darker and more reddish than the unsteamed one. An imprecision of measurement by probes in the kiln was noticed in measuring steamed and unsteamed beech timber having a moisture content of between 7% and 15%, and a solution for overcoming this problem was given.
PB  - Univerzitet u Beogradu - Šumarski fakultet, Beograd
T2  - Glasnik Šumarskog fakulteta
T1  - Uticaj parenja na kvalitet sušenja i boju rezane građe bukve
T1  - Influence of steaming on drying quality and colour of beech timber
EP  - 95
IS  - 112
SP  - 83
DO  - 10.2298/GSF1512083M
UR  - conv_431
ER  - 
@article{
author = "Milić, Goran and Todorović, Nebojša and Popadić, Ranko",
year = "2015",
abstract = "U radu su prikazani rezultati analize uticaja tzv. blagog parenja na konvencionalno sušenje i boju tako osušene rezane građe bukve. Osušena je šarža koja se sastojala od parenih i neparenih dasaka. Praćeni su vlažnost i profili vlažnosti tokom sušenja, a na kraju sušenja su određivani konačna vlažnost, razlika vlažnosti po debljini građe, skorelost i boja. Statistički značajna razlika između parene i neparene građe nije utvrđena ni kod jednog ispitivanog parametra. Rezultati pokazuju da se može očekivati isti (ili čak bolji) kvalitet sušenja parene bukove građe u odnosu na neparenu sušenu istim režimom. Osušena parena rezana građa je imala tamniju boju sa većim učešćem crvene u odnosu na neparenu građu. Utvrđena je nepreciznost merenja vlažnosti parenog i neparenog drveta bukve u sušari u području vlažnosti 7-15% i data preporuka za prevazilaženje ovog problema., This paper presents the results of an analysis of influence of the 'light' steaming process on conventional drying and colour of beech timber. A stack consisting of steamed and unsteamed boards was dried. Moisture content and moisture content profiles were recorded, and at the end of drying final moisture content, moisture content difference across thickness, case-hardening and colour were determinated. No statistically significant difference between steamed and unsteamed timber was established in any of the examined parameters (MC, ΔMC, gap). The results indicate that equal (or even) better drying quality can be expected with steamed beech timber than with unsteamed timber, given the same drying schedule. Dry steamed timber was darker and more reddish than the unsteamed one. An imprecision of measurement by probes in the kiln was noticed in measuring steamed and unsteamed beech timber having a moisture content of between 7% and 15%, and a solution for overcoming this problem was given.",
publisher = "Univerzitet u Beogradu - Šumarski fakultet, Beograd",
journal = "Glasnik Šumarskog fakulteta",
title = "Uticaj parenja na kvalitet sušenja i boju rezane građe bukve, Influence of steaming on drying quality and colour of beech timber",
pages = "95-83",
number = "112",
doi = "10.2298/GSF1512083M",
url = "conv_431"
}
Milić, G., Todorović, N.,& Popadić, R.. (2015). Uticaj parenja na kvalitet sušenja i boju rezane građe bukve. in Glasnik Šumarskog fakulteta
Univerzitet u Beogradu - Šumarski fakultet, Beograd.(112), 83-95.
https://doi.org/10.2298/GSF1512083M
conv_431
Milić G, Todorović N, Popadić R. Uticaj parenja na kvalitet sušenja i boju rezane građe bukve. in Glasnik Šumarskog fakulteta. 2015;(112):83-95.
doi:10.2298/GSF1512083M
conv_431 .
Milić, Goran, Todorović, Nebojša, Popadić, Ranko, "Uticaj parenja na kvalitet sušenja i boju rezane građe bukve" in Glasnik Šumarskog fakulteta, no. 112 (2015):83-95,
https://doi.org/10.2298/GSF1512083M .,
conv_431 .
8

Estimation of quality of thermally modified beech wood with red heartwood by FT-NIR spectroscopy

Todorović, Nebojša; Popović, Zdravko; Milić, Goran

(2015)

TY  - JOUR
AU  - Todorović, Nebojša
AU  - Popović, Zdravko
AU  - Milić, Goran
PY  - 2015
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/642
AB  - The research examines the possibility of predicting the mechanical [modulus of rupture (MOR) and modulus of elasticity (MOE)] and physical (oven-dry and air-dry densities) properties of thermally modified beech wood (Fagus moesica C.) with red heartwood by using FT-NIR spectroscopy and partial least squares regression. Samples of sapwood and red heartwood were treated for 4 h at temperatures of 170, 190, and 210 A degrees C. FT-NIR spectra (100 scans and 4 cm(-1)) were collected on the radial surface at eight points before and after the thermal modification. Oven-dry and air-dry densities as well as MOR and MOE determined by three-point bending tests were evaluated. Generally, according to the residual prediction deviation (RPD), the majority of the models obtained can be used for preliminary screening (1.5  lt  RPD  lt  2.5). The results of the spectra taken from sapwood were, in most models, better than the spectra of the red heartwood. Statistically, the values of density were mostly better than the values shown in assessment of bending properties. Results show that it is possible to accurately predict the quality of wood after being subjected to high temperatures, based on the spectra collected before the thermal modification. This fact could contribute to a more rational use of wood (especially from red heartwood) in the process of thermal modification.
T2  - Wood Science and Technology
T1  - Estimation of quality of thermally modified beech wood with red heartwood by FT-NIR spectroscopy
EP  - 549
IS  - 3
SP  - 527
VL  - 49
DO  - 10.1007/s00226-015-0710-3
UR  - conv_1156
ER  - 
@article{
author = "Todorović, Nebojša and Popović, Zdravko and Milić, Goran",
year = "2015",
abstract = "The research examines the possibility of predicting the mechanical [modulus of rupture (MOR) and modulus of elasticity (MOE)] and physical (oven-dry and air-dry densities) properties of thermally modified beech wood (Fagus moesica C.) with red heartwood by using FT-NIR spectroscopy and partial least squares regression. Samples of sapwood and red heartwood were treated for 4 h at temperatures of 170, 190, and 210 A degrees C. FT-NIR spectra (100 scans and 4 cm(-1)) were collected on the radial surface at eight points before and after the thermal modification. Oven-dry and air-dry densities as well as MOR and MOE determined by three-point bending tests were evaluated. Generally, according to the residual prediction deviation (RPD), the majority of the models obtained can be used for preliminary screening (1.5  lt  RPD  lt  2.5). The results of the spectra taken from sapwood were, in most models, better than the spectra of the red heartwood. Statistically, the values of density were mostly better than the values shown in assessment of bending properties. Results show that it is possible to accurately predict the quality of wood after being subjected to high temperatures, based on the spectra collected before the thermal modification. This fact could contribute to a more rational use of wood (especially from red heartwood) in the process of thermal modification.",
journal = "Wood Science and Technology",
title = "Estimation of quality of thermally modified beech wood with red heartwood by FT-NIR spectroscopy",
pages = "549-527",
number = "3",
volume = "49",
doi = "10.1007/s00226-015-0710-3",
url = "conv_1156"
}
Todorović, N., Popović, Z.,& Milić, G.. (2015). Estimation of quality of thermally modified beech wood with red heartwood by FT-NIR spectroscopy. in Wood Science and Technology, 49(3), 527-549.
https://doi.org/10.1007/s00226-015-0710-3
conv_1156
Todorović N, Popović Z, Milić G. Estimation of quality of thermally modified beech wood with red heartwood by FT-NIR spectroscopy. in Wood Science and Technology. 2015;49(3):527-549.
doi:10.1007/s00226-015-0710-3
conv_1156 .
Todorović, Nebojša, Popović, Zdravko, Milić, Goran, "Estimation of quality of thermally modified beech wood with red heartwood by FT-NIR spectroscopy" in Wood Science and Technology, 49, no. 3 (2015):527-549,
https://doi.org/10.1007/s00226-015-0710-3 .,
conv_1156 .
30
35
38

Influence of the Sawing Method on Yield of Beech Logs with Red Heartwood

Popadić, Ranko; Šoškić, Borislav; Milić, Goran; Todorović, Nebojša; Furtula, Mladen

(2014)

TY  - JOUR
AU  - Popadić, Ranko
AU  - Šoškić, Borislav
AU  - Milić, Goran
AU  - Todorović, Nebojša
AU  - Furtula, Mladen
PY  - 2014
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/583
AB  - The paper presents the research of differences in quantitative and value yields, and structure of sawn timber and residues, whose appearance is caused by different methods of sawing beech logs with red heartwood. In order to achieve the goal, 45 logs were divided into three even groups and sawn into commercial timber using three methods: round, cant and live sawing. Similar quantitative yields were found for round sawing and cant sawing (60.63 % and 60.52 %, respectively), while a lower result of 56.79 % was observed for live sawing. Less timber ( edged and red heartwood boards) and smaller products were found in live sawing than in other two methods, meaning that live sawing resulted in a lower value yield.
T2  - Drvna industrija
T1  - Influence of the Sawing Method on Yield of Beech Logs with Red Heartwood
EP  - 42
IS  - 1
SP  - 35
VL  - 65
DO  - 10.5552/drind.2014.1312
UR  - conv_1113
ER  - 
@article{
author = "Popadić, Ranko and Šoškić, Borislav and Milić, Goran and Todorović, Nebojša and Furtula, Mladen",
year = "2014",
abstract = "The paper presents the research of differences in quantitative and value yields, and structure of sawn timber and residues, whose appearance is caused by different methods of sawing beech logs with red heartwood. In order to achieve the goal, 45 logs were divided into three even groups and sawn into commercial timber using three methods: round, cant and live sawing. Similar quantitative yields were found for round sawing and cant sawing (60.63 % and 60.52 %, respectively), while a lower result of 56.79 % was observed for live sawing. Less timber ( edged and red heartwood boards) and smaller products were found in live sawing than in other two methods, meaning that live sawing resulted in a lower value yield.",
journal = "Drvna industrija",
title = "Influence of the Sawing Method on Yield of Beech Logs with Red Heartwood",
pages = "42-35",
number = "1",
volume = "65",
doi = "10.5552/drind.2014.1312",
url = "conv_1113"
}
Popadić, R., Šoškić, B., Milić, G., Todorović, N.,& Furtula, M.. (2014). Influence of the Sawing Method on Yield of Beech Logs with Red Heartwood. in Drvna industrija, 65(1), 35-42.
https://doi.org/10.5552/drind.2014.1312
conv_1113
Popadić R, Šoškić B, Milić G, Todorović N, Furtula M. Influence of the Sawing Method on Yield of Beech Logs with Red Heartwood. in Drvna industrija. 2014;65(1):35-42.
doi:10.5552/drind.2014.1312
conv_1113 .
Popadić, Ranko, Šoškić, Borislav, Milić, Goran, Todorović, Nebojša, Furtula, Mladen, "Influence of the Sawing Method on Yield of Beech Logs with Red Heartwood" in Drvna industrija, 65, no. 1 (2014):35-42,
https://doi.org/10.5552/drind.2014.1312 .,
conv_1113 .
11
10
9

Energy Consumption of Beech Timber Drying in Oscillation Climates

Milić, Goran; Kolin, Branko; Todorović, Nebojša; Gorisek, Zeljko

(2014)

TY  - JOUR
AU  - Milić, Goran
AU  - Kolin, Branko
AU  - Todorović, Nebojša
AU  - Gorisek, Zeljko
PY  - 2014
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/568
AB  - The influence of applying the oscillations of air parameters during conventional drying of beech timber on energy consumption is discussed in the paper. A special drying software was created to enable the input of frequency (in hours) and amplitude (in percents) of oscillations. Altogether 12 drying runs were carried out: three conventional ones and nine by using the same schedule but with oscillations of equilibrium moisture content (EMC), temperature and the combination of these two. The combinations of two amplitudes (10 % or 20 %) and two frequencies (3 or 6 hours) were applied in different test runs. The results indicated that all test runs had energy consumptions proportional to drying time, with an important influence of the outside temperature. In runs with oscillations, often climate changes influenced to some extent the total energy consumption, especially in runs with short phases (3 hours) and high amplitudes (20 %). Despite frequent climate changes, it can be expected that the usage of oscillations would lead to the same or even lower energy consumption than in conventional beech timber drying, especially when shorter drying time is reached.
T2  - Drvna industrija
T1  - Energy Consumption of Beech Timber Drying in Oscillation Climates
EP  - 314
IS  - 4
SP  - 309
VL  - 65
DO  - 10.5552/drind.2014.1367
UR  - conv_1145
ER  - 
@article{
author = "Milić, Goran and Kolin, Branko and Todorović, Nebojša and Gorisek, Zeljko",
year = "2014",
abstract = "The influence of applying the oscillations of air parameters during conventional drying of beech timber on energy consumption is discussed in the paper. A special drying software was created to enable the input of frequency (in hours) and amplitude (in percents) of oscillations. Altogether 12 drying runs were carried out: three conventional ones and nine by using the same schedule but with oscillations of equilibrium moisture content (EMC), temperature and the combination of these two. The combinations of two amplitudes (10 % or 20 %) and two frequencies (3 or 6 hours) were applied in different test runs. The results indicated that all test runs had energy consumptions proportional to drying time, with an important influence of the outside temperature. In runs with oscillations, often climate changes influenced to some extent the total energy consumption, especially in runs with short phases (3 hours) and high amplitudes (20 %). Despite frequent climate changes, it can be expected that the usage of oscillations would lead to the same or even lower energy consumption than in conventional beech timber drying, especially when shorter drying time is reached.",
journal = "Drvna industrija",
title = "Energy Consumption of Beech Timber Drying in Oscillation Climates",
pages = "314-309",
number = "4",
volume = "65",
doi = "10.5552/drind.2014.1367",
url = "conv_1145"
}
Milić, G., Kolin, B., Todorović, N.,& Gorisek, Z.. (2014). Energy Consumption of Beech Timber Drying in Oscillation Climates. in Drvna industrija, 65(4), 309-314.
https://doi.org/10.5552/drind.2014.1367
conv_1145
Milić G, Kolin B, Todorović N, Gorisek Z. Energy Consumption of Beech Timber Drying in Oscillation Climates. in Drvna industrija. 2014;65(4):309-314.
doi:10.5552/drind.2014.1367
conv_1145 .
Milić, Goran, Kolin, Branko, Todorović, Nebojša, Gorisek, Zeljko, "Energy Consumption of Beech Timber Drying in Oscillation Climates" in Drvna industrija, 65, no. 4 (2014):309-314,
https://doi.org/10.5552/drind.2014.1367 .,
conv_1145 .
9
7
6

Drying of beech ( Fagus sylvatica L.) timber in oscillation climates: drying time and quality

Milić, Goran; Kolin, Branko; Lovrić, Aleksandar; Todorović, Nebojša; Popadić, Ranko

(2013)

TY  - JOUR
AU  - Milić, Goran
AU  - Kolin, Branko
AU  - Lovrić, Aleksandar
AU  - Todorović, Nebojša
AU  - Popadić, Ranko
PY  - 2013
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/554
AB  - The influence of oscillating climate conditions during the conventional drying of beech timber on drying time and drying quality has been analyzed. Three conventional drying cycles were carried out as well as nine cycles, in which the oscillations of equilibrium moisture content (EMC), temperature, and their combination were applied. The combinations of two amplitudes (10% or 20%) and two frequencies (3 or 6 h) were used in different test runs. Higher drying quality regarding casehardening was achieved both in runs with oscillations of EMC (gap values 2.2-2.4 mm) and in runs with temperature oscillations (gap values 2.3-2.4 mm) compared with conventional runs (gap values 2.5-2.9 mm). The oscillations of both temperature and EMC did not improve any of the observed parameters.
T2  - Holzforschung
T1  - Drying of beech ( Fagus sylvatica L.) timber in oscillation climates: drying time and quality
EP  - 813
IS  - 7
SP  - 805
VL  - 67
DO  - 10.1515/hf-2012-0203
UR  - conv_1103
ER  - 
@article{
author = "Milić, Goran and Kolin, Branko and Lovrić, Aleksandar and Todorović, Nebojša and Popadić, Ranko",
year = "2013",
abstract = "The influence of oscillating climate conditions during the conventional drying of beech timber on drying time and drying quality has been analyzed. Three conventional drying cycles were carried out as well as nine cycles, in which the oscillations of equilibrium moisture content (EMC), temperature, and their combination were applied. The combinations of two amplitudes (10% or 20%) and two frequencies (3 or 6 h) were used in different test runs. Higher drying quality regarding casehardening was achieved both in runs with oscillations of EMC (gap values 2.2-2.4 mm) and in runs with temperature oscillations (gap values 2.3-2.4 mm) compared with conventional runs (gap values 2.5-2.9 mm). The oscillations of both temperature and EMC did not improve any of the observed parameters.",
journal = "Holzforschung",
title = "Drying of beech ( Fagus sylvatica L.) timber in oscillation climates: drying time and quality",
pages = "813-805",
number = "7",
volume = "67",
doi = "10.1515/hf-2012-0203",
url = "conv_1103"
}
Milić, G., Kolin, B., Lovrić, A., Todorović, N.,& Popadić, R.. (2013). Drying of beech ( Fagus sylvatica L.) timber in oscillation climates: drying time and quality. in Holzforschung, 67(7), 805-813.
https://doi.org/10.1515/hf-2012-0203
conv_1103
Milić G, Kolin B, Lovrić A, Todorović N, Popadić R. Drying of beech ( Fagus sylvatica L.) timber in oscillation climates: drying time and quality. in Holzforschung. 2013;67(7):805-813.
doi:10.1515/hf-2012-0203
conv_1103 .
Milić, Goran, Kolin, Branko, Lovrić, Aleksandar, Todorović, Nebojša, Popadić, Ranko, "Drying of beech ( Fagus sylvatica L.) timber in oscillation climates: drying time and quality" in Holzforschung, 67, no. 7 (2013):805-813,
https://doi.org/10.1515/hf-2012-0203 .,
conv_1103 .
9
9
8

Estimation of heat-treated beechwood properties by color change

Todorović, Nebojša; Popović, Zdravko; Milić, Goran; Popadić, Ranko

(North Carolina State University, 2012)

TY  - JOUR
AU  - Todorović, Nebojša
AU  - Popović, Zdravko
AU  - Milić, Goran
AU  - Popadić, Ranko
PY  - 2012
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/474
AB  - Changes in color (CIE L*a*b*) and properties (density, mass loss, density loss, and bending properties) of heat-treated beechwood were researched, as well as the possibilities of predicting these properties based on color. Considering the different market values of sapwood and red heartwood, the aim of this study was to establish whether these parts of beechwood differ after a heat treatment. Samples were exposed to temperatures of 170 degrees C, 190 degrees C, and 210 degrees C, respectively, for 4 hours. In order to predict the properties, a linear regression with color change (Delta E) and Delta L predictors was used, as well as the partial least squares (PLS) regression with 12 color variables. It has been shown that heat treatment reduces the properties of sapwood and red heartwood in the same manner, and equalizes the colors. The PLS-R showed the best results of prediction and presented the very high coefficients of determination for the mass loss, density loss, and modulus of rupture (MOR) in both sapwood and red heartwood. The equalized colors of heat- treated red heartwood and sapwood can significantly increase the use of products made out of red heartwood. Color can be an important indicator of the quality of such beechwood.
PB  - North Carolina State University
T2  - BioResources
T1  - Estimation of heat-treated beechwood properties by color change
EP  - 815
IS  - 1
SP  - 799
VL  - 7
DO  - 10.15376/biores.7.1.799-815
UR  - conv_2185
ER  - 
@article{
author = "Todorović, Nebojša and Popović, Zdravko and Milić, Goran and Popadić, Ranko",
year = "2012",
abstract = "Changes in color (CIE L*a*b*) and properties (density, mass loss, density loss, and bending properties) of heat-treated beechwood were researched, as well as the possibilities of predicting these properties based on color. Considering the different market values of sapwood and red heartwood, the aim of this study was to establish whether these parts of beechwood differ after a heat treatment. Samples were exposed to temperatures of 170 degrees C, 190 degrees C, and 210 degrees C, respectively, for 4 hours. In order to predict the properties, a linear regression with color change (Delta E) and Delta L predictors was used, as well as the partial least squares (PLS) regression with 12 color variables. It has been shown that heat treatment reduces the properties of sapwood and red heartwood in the same manner, and equalizes the colors. The PLS-R showed the best results of prediction and presented the very high coefficients of determination for the mass loss, density loss, and modulus of rupture (MOR) in both sapwood and red heartwood. The equalized colors of heat- treated red heartwood and sapwood can significantly increase the use of products made out of red heartwood. Color can be an important indicator of the quality of such beechwood.",
publisher = "North Carolina State University",
journal = "BioResources",
title = "Estimation of heat-treated beechwood properties by color change",
pages = "815-799",
number = "1",
volume = "7",
doi = "10.15376/biores.7.1.799-815",
url = "conv_2185"
}
Todorović, N., Popović, Z., Milić, G.,& Popadić, R.. (2012). Estimation of heat-treated beechwood properties by color change. in BioResources
North Carolina State University., 7(1), 799-815.
https://doi.org/10.15376/biores.7.1.799-815
conv_2185
Todorović N, Popović Z, Milić G, Popadić R. Estimation of heat-treated beechwood properties by color change. in BioResources. 2012;7(1):799-815.
doi:10.15376/biores.7.1.799-815
conv_2185 .
Todorović, Nebojša, Popović, Zdravko, Milić, Goran, Popadić, Ranko, "Estimation of heat-treated beechwood properties by color change" in BioResources, 7, no. 1 (2012):799-815,
https://doi.org/10.15376/biores.7.1.799-815 .,
conv_2185 .
48

Brzina i ravnomernost cirkulacije vazduha u konvencionalnim komornim sušarama za rezanu građu

Kolin, Branko; Milić, Goran; Golić, Igor

(Univerzitet u Beogradu - Šumarski fakultet, Beograd, 2012)

TY  - JOUR
AU  - Kolin, Branko
AU  - Milić, Goran
AU  - Golić, Igor
PY  - 2012
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/444
AB  - U radu su prikazani rezultati istraživanja brzine cirkulacije vazduha u konvencionalnim komornim sušarama za rezanu građu i njihov uticaj na ravnomernost konačne vlažnosti. Dobijeni podaci pokazuju da su brzine vazduha (između 0.8 - 1.2 m·s-1) značajno manje od onih koje su optimalne za sušenje rezane građe četinara ( 3 - 4 m·s-1). Ovo za posledicu ima smanjenje kapaciteta instalacije za sušenje, povećanje potrošnje energije (toplotne i električne), a samim tim i povećanje cene sušenja. Nije ustanovljena korelaciona zavisnost između brzine cirkulacije vazduha i konačne vlažnosti građe usled produženog trajanja sušenja.U radu su dati predlozi mera za otklanjanje utvrđenih nedostataka.
AB  - This paper presents the results of a research of velocity of air circulation in the conventional kiln drying of sawn timber and its influence on the uniformity of final moisture content. The data showed that the air velocity (between 0.8 - 1.2 m·s -1) is significantly lower than the one that is optimal for timber drying of coniferous species (3 - 4 m·s-1). This results in a reduction in the capacity of installations for drying, increased energy (thermal and electrical) consumption and thereby increase in the cost of drying. The correlation between the speed of air circulation and the final MC of timber due to prolonged drying was not established. Recommendations that should eliminate the identified deficiencies are also given.
PB  - Univerzitet u Beogradu - Šumarski fakultet, Beograd
T2  - Glasnik Šumarskog fakulteta
T1  - Brzina i ravnomernost cirkulacije vazduha u konvencionalnim komornim sušarama za rezanu građu
T1  - Velocity and uniformity of air circulation in conventional kilns for sawn timber
EP  - 140
IS  - 106
SP  - 129
DO  - 10.2298/GSF1206129K
UR  - conv_374
ER  - 
@article{
author = "Kolin, Branko and Milić, Goran and Golić, Igor",
year = "2012",
abstract = "U radu su prikazani rezultati istraživanja brzine cirkulacije vazduha u konvencionalnim komornim sušarama za rezanu građu i njihov uticaj na ravnomernost konačne vlažnosti. Dobijeni podaci pokazuju da su brzine vazduha (između 0.8 - 1.2 m·s-1) značajno manje od onih koje su optimalne za sušenje rezane građe četinara ( 3 - 4 m·s-1). Ovo za posledicu ima smanjenje kapaciteta instalacije za sušenje, povećanje potrošnje energije (toplotne i električne), a samim tim i povećanje cene sušenja. Nije ustanovljena korelaciona zavisnost između brzine cirkulacije vazduha i konačne vlažnosti građe usled produženog trajanja sušenja.U radu su dati predlozi mera za otklanjanje utvrđenih nedostataka., This paper presents the results of a research of velocity of air circulation in the conventional kiln drying of sawn timber and its influence on the uniformity of final moisture content. The data showed that the air velocity (between 0.8 - 1.2 m·s -1) is significantly lower than the one that is optimal for timber drying of coniferous species (3 - 4 m·s-1). This results in a reduction in the capacity of installations for drying, increased energy (thermal and electrical) consumption and thereby increase in the cost of drying. The correlation between the speed of air circulation and the final MC of timber due to prolonged drying was not established. Recommendations that should eliminate the identified deficiencies are also given.",
publisher = "Univerzitet u Beogradu - Šumarski fakultet, Beograd",
journal = "Glasnik Šumarskog fakulteta",
title = "Brzina i ravnomernost cirkulacije vazduha u konvencionalnim komornim sušarama za rezanu građu, Velocity and uniformity of air circulation in conventional kilns for sawn timber",
pages = "140-129",
number = "106",
doi = "10.2298/GSF1206129K",
url = "conv_374"
}
Kolin, B., Milić, G.,& Golić, I.. (2012). Brzina i ravnomernost cirkulacije vazduha u konvencionalnim komornim sušarama za rezanu građu. in Glasnik Šumarskog fakulteta
Univerzitet u Beogradu - Šumarski fakultet, Beograd.(106), 129-140.
https://doi.org/10.2298/GSF1206129K
conv_374
Kolin B, Milić G, Golić I. Brzina i ravnomernost cirkulacije vazduha u konvencionalnim komornim sušarama za rezanu građu. in Glasnik Šumarskog fakulteta. 2012;(106):129-140.
doi:10.2298/GSF1206129K
conv_374 .
Kolin, Branko, Milić, Goran, Golić, Igor, "Brzina i ravnomernost cirkulacije vazduha u konvencionalnim komornim sušarama za rezanu građu" in Glasnik Šumarskog fakulteta, no. 106 (2012):129-140,
https://doi.org/10.2298/GSF1206129K .,
conv_374 .

Moisture content distribution across thickness of kiln dried oak and beech lumber during conditioning phase

Milić, Goran; Kolin, B.

(2008)

TY  - JOUR
AU  - Milić, Goran
AU  - Kolin, B.
PY  - 2008
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/227
AB  - The research results of measuring and analyzing moisture content distribution across thickness of oak and beech lumber during the conditioning phase are presented. Moisture content difference between the core and the surface layers of wood was reduced during conditioning due to the increase of moisture in the surface layers. It was shown that by means of conditioning it was possible for both species oak and beech to reach the highest drying quality conforming to the European Drying Group (EDG) Recommendation even in shorter times than usually needed for oak, 25 mm thick. The conditioning regimes, using EMC that is lower than final MC, will not give adequate results of conditioning. The drying schedule has a relevant influence on moisture content distribution prior to the conditioning phase. Therefore, the time of conditioning depends on the drying schedule and the required drying quality. Other parameters that influence drying quality (final moisture content, casehardening) should also be considered.
T2  - HOLZ ALS ROH-UND WERKSTOFF
T1  - Moisture content distribution across thickness of kiln dried oak and beech lumber during conditioning phase
EP  - 87
IS  - 2
SP  - 83
VL  - 66
DO  - 10.1007/s00107-007-0206-4
UR  - conv_871
ER  - 
@article{
author = "Milić, Goran and Kolin, B.",
year = "2008",
abstract = "The research results of measuring and analyzing moisture content distribution across thickness of oak and beech lumber during the conditioning phase are presented. Moisture content difference between the core and the surface layers of wood was reduced during conditioning due to the increase of moisture in the surface layers. It was shown that by means of conditioning it was possible for both species oak and beech to reach the highest drying quality conforming to the European Drying Group (EDG) Recommendation even in shorter times than usually needed for oak, 25 mm thick. The conditioning regimes, using EMC that is lower than final MC, will not give adequate results of conditioning. The drying schedule has a relevant influence on moisture content distribution prior to the conditioning phase. Therefore, the time of conditioning depends on the drying schedule and the required drying quality. Other parameters that influence drying quality (final moisture content, casehardening) should also be considered.",
journal = "HOLZ ALS ROH-UND WERKSTOFF",
title = "Moisture content distribution across thickness of kiln dried oak and beech lumber during conditioning phase",
pages = "87-83",
number = "2",
volume = "66",
doi = "10.1007/s00107-007-0206-4",
url = "conv_871"
}
Milić, G.,& Kolin, B.. (2008). Moisture content distribution across thickness of kiln dried oak and beech lumber during conditioning phase. in HOLZ ALS ROH-UND WERKSTOFF, 66(2), 83-87.
https://doi.org/10.1007/s00107-007-0206-4
conv_871
Milić G, Kolin B. Moisture content distribution across thickness of kiln dried oak and beech lumber during conditioning phase. in HOLZ ALS ROH-UND WERKSTOFF. 2008;66(2):83-87.
doi:10.1007/s00107-007-0206-4
conv_871 .
Milić, Goran, Kolin, B., "Moisture content distribution across thickness of kiln dried oak and beech lumber during conditioning phase" in HOLZ ALS ROH-UND WERKSTOFF, 66, no. 2 (2008):83-87,
https://doi.org/10.1007/s00107-007-0206-4 .,
conv_871 .
6
5
5

Influence of duration of the conditioning process on the reduction of case-hardening level in kiln-dried beech and oak lumber

Milić, Goran; Kolin, Branko

(2008)

TY  - JOUR
AU  - Milić, Goran
AU  - Kolin, Branko
PY  - 2008
UR  - https://omorika.sfb.bg.ac.rs/handle/123456789/223
AB  - The research results from an analysis of the influence of conditioning time on case-hardening reduction are presented. The levels of case-hardening and moisture content differences across the thickness on beech and oak lumber were measured before, during, and after conditioning. A relationship between gap, as the measure of case-hardening in wood (ENV 14464), and conditioning time was found; a highly linear relationship also exists between gap and moisture content differences across the lumber thickness. Time analysis showed that much shorter conditioning times were adequate to reach acceptable drying quality than the times currently used. It is shown that the conditioning regimes that use equilibrium moisture content lower than the final moisture content are inadequate to obtain a dried product quality that meets modern European standards.
T2  - Drying Technology
T1  - Influence of duration of the conditioning process on the reduction of case-hardening level in kiln-dried beech and oak lumber
EP  - 1231
IS  - 10
SP  - 1225
VL  - 26
DO  - 10.1080/07373930802307035
UR  - conv_882
ER  - 
@article{
author = "Milić, Goran and Kolin, Branko",
year = "2008",
abstract = "The research results from an analysis of the influence of conditioning time on case-hardening reduction are presented. The levels of case-hardening and moisture content differences across the thickness on beech and oak lumber were measured before, during, and after conditioning. A relationship between gap, as the measure of case-hardening in wood (ENV 14464), and conditioning time was found; a highly linear relationship also exists between gap and moisture content differences across the lumber thickness. Time analysis showed that much shorter conditioning times were adequate to reach acceptable drying quality than the times currently used. It is shown that the conditioning regimes that use equilibrium moisture content lower than the final moisture content are inadequate to obtain a dried product quality that meets modern European standards.",
journal = "Drying Technology",
title = "Influence of duration of the conditioning process on the reduction of case-hardening level in kiln-dried beech and oak lumber",
pages = "1231-1225",
number = "10",
volume = "26",
doi = "10.1080/07373930802307035",
url = "conv_882"
}
Milić, G.,& Kolin, B.. (2008). Influence of duration of the conditioning process on the reduction of case-hardening level in kiln-dried beech and oak lumber. in Drying Technology, 26(10), 1225-1231.
https://doi.org/10.1080/07373930802307035
conv_882
Milić G, Kolin B. Influence of duration of the conditioning process on the reduction of case-hardening level in kiln-dried beech and oak lumber. in Drying Technology. 2008;26(10):1225-1231.
doi:10.1080/07373930802307035
conv_882 .
Milić, Goran, Kolin, Branko, "Influence of duration of the conditioning process on the reduction of case-hardening level in kiln-dried beech and oak lumber" in Drying Technology, 26, no. 10 (2008):1225-1231,
https://doi.org/10.1080/07373930802307035 .,
conv_882 .
8
7
8